Final Magnetic Moment9.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.389 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV3O5 + Li3VO4 + Fe2O3 + V2O3 |
Band Gap1.161 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP43212 [96] |
HallP 4nw 2abw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <0 0 1> | 212.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 215.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 101.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 215.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 203.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 287.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 287.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 283.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 143.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 212.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 141.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 283.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 1> | 201.8 |
TeO2 (mp-2125) | <1 0 0> | <1 0 1> | 201.8 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 287.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 283.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 287.3 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 123.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 143.6 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 247.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 287.3 |
C (mp-66) | <1 1 0> | <1 0 1> | 201.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 287.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 212.7 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 70.9 |
InP (mp-20351) | <1 1 0> | <1 0 1> | 100.9 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 212.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 141.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 70.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 1> | 100.9 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 123.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 70.9 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 100.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 283.6 |
C (mp-66) | <1 1 1> | <1 0 0> | 215.4 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 283.6 |
PbS (mp-21276) | <1 1 0> | <1 0 1> | 100.9 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 283.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 70.9 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 283.6 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 1> | 100.9 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 283.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 141.8 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 283.6 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 1> | 123.9 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 215.4 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 143.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 70.9 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 215.4 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 71.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(CuO2)2 (mvc-5434) | 0.1546 | 0.074 | 3 |
MgMn2O4 (mvc-5228) | 0.1219 | 1.184 | 3 |
LiCr2O4 (mp-774032) | 0.1355 | 0.048 | 3 |
Mg2TiO4 (mp-677628) | 0.1550 | 0.033 | 3 |
Mg(NiO2)2 (mvc-12526) | 0.1545 | 0.034 | 3 |
Li2V3SnO8 (mp-774164) | 0.1123 | 0.027 | 4 |
Li2Cr3FeO8 (mp-777653) | 0.1021 | 0.860 | 4 |
Li2TiV3O8 (mp-775564) | 0.0925 | 0.043 | 4 |
Li2Cr3SnO8 (mp-774276) | 0.1073 | 0.052 | 4 |
Li2V3CrO8 (mp-774288) | 0.0844 | 0.003 | 4 |
Fe3O4 (mp-715491) | 0.2698 | 0.017 | 2 |
In3S4 (mp-556597) | 0.3002 | 0.042 | 2 |
Ni3S4 (mp-1050) | 0.2793 | 0.000 | 2 |
Fe3O4 (mp-650112) | 0.2819 | 0.060 | 2 |
Fe3O4 (mp-31770) | 0.2800 | 0.017 | 2 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.2094 | 0.078 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.1815 | 0.014 | 5 |
Li4Ti3Cr3(WO8)2 (mp-773537) | 0.2075 | 0.054 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.2074 | 0.069 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.2015 | 0.035 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6835 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6870 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6936 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6881 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6907 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv O |
Final Energy/Atom-7.0829 eV |
Corrected Energy-448.0518 eV
Uncorrected energy = -396.6438 eV
Composition-based energy adjustment (-0.687 eV/atom x 32.0 atoms) = -21.9840 eV
Composition-based energy adjustment (-1.700 eV/atom x 12.0 atoms) = -20.4000 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -448.0518 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)