Final Magnetic Moment0.300 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.051 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3Ni2P2(CO7)2 + Na3NiPCO7 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 204.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 287.5 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 68.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 261.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 273.1 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 261.0 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 273.1 |
GaSe (mp-1943) | <1 0 1> | <0 1 -1> | 275.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 287.5 |
BN (mp-984) | <1 1 0> | <0 1 -1> | 275.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 68.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 342.0 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 204.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 342.0 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 136.6 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 204.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 -1> | 275.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 287.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 204.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 285.0 |
Al (mp-134) | <1 0 0> | <0 1 1> | 273.1 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 273.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 285.0 |
MgO (mp-1265) | <1 1 1> | <0 1 1> | 273.1 |
TiO2 (mp-2657) | <1 0 0> | <0 1 -1> | 275.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 285.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 118.4 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 118.4 |
C (mp-66) | <1 0 0> | <0 1 1> | 204.8 |
C (mp-66) | <1 1 0> | <0 1 1> | 273.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 285.0 |
Au (mp-81) | <1 1 1> | <0 1 1> | 273.1 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 285.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 228.0 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 204.8 |
C (mp-48) | <1 0 1> | <0 0 1> | 285.0 |
WSe2 (mp-1821) | <1 0 0> | <0 1 1> | 204.8 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 1> | 136.6 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 -1> | 275.7 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 -1> | 275.7 |
LaF3 (mp-905) | <1 0 0> | <0 1 1> | 273.1 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 1> | 204.8 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 1> | 135.0 |
GaP (mp-2490) | <1 1 1> | <0 1 1> | 204.8 |
CaCO3 (mp-3953) | <1 0 0> | <0 1 1> | 273.1 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 -1> | 275.7 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 1> | 136.6 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 273.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 1> | 273.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 1> | 273.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiSn10(PO4)7 (mp-765193) | 0.7120 | 0.086 | 4 |
Na2NiPCO7 (mp-768070) | 0.1252 | 0.050 | 5 |
Na2NiPCO7 (mp-775513) | 0.1526 | 0.076 | 5 |
Na2NiPCO7 (mp-775473) | 0.1245 | 0.055 | 5 |
Na2NiPCO7 (mp-769501) | 0.1529 | 0.073 | 5 |
Na2NiPCO7 (mp-769504) | 0.1244 | 0.049 | 5 |
Na5LiCo2P2(CO7)2 (mp-761297) | 0.5364 | 0.013 | 6 |
Na5LiCo2P2(CO7)2 (mp-770326) | 0.5638 | 0.011 | 6 |
Na5LiNi2P2(CO7)2 (mp-770324) | 0.4481 | 0.009 | 6 |
Na2LiFePCO7 (mp-773705) | 0.5035 | 0.138 | 6 |
Na5LiNi2P2(CO7)2 (mp-771060) | 0.5295 | 0.011 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Na_pv Ni_pv P C O |
Final Energy/Atom-6.2679 eV |
Corrected Energy-329.1813 eV
-329.1813 eV = -300.8612 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)