Final Magnetic Moment8.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.398 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.094 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn2P2O7 + MnPO4 + SnP2O7 + SnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [167] |
Hall-R 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 201.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 195.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 269.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 67.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 201.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 269.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 201.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 201.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 201.9 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 195.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 269.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 67.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 269.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 269.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 269.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 201.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 67.3 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 269.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 269.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 67.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 201.9 |
Si (mp-149) | <1 1 1> | <0 0 1> | 201.9 |
Au (mp-81) | <1 1 1> | <0 0 1> | 269.2 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 195.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 201.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 67.3 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 269.2 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 67.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 201.9 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 67.3 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 269.2 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 269.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 201.9 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 1> | 195.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 67.3 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 269.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 201.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 269.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 201.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 269.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 67.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 269.2 |
GaSb (mp-1156) | <1 0 0> | <1 0 1> | 195.3 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 269.2 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 67.3 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 67.3 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 201.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
VPO4 (mp-861584) | 0.4174 | 0.079 | 3 |
FePO4 (mp-773675) | 0.2166 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.3582 | 0.077 | 3 |
TiPO4 (mp-25435) | 0.4729 | 0.128 | 3 |
VPO4 (mp-32453) | 0.4689 | 0.112 | 3 |
VFe2(PO4)3 (mp-851013) | 0.2062 | 0.371 | 4 |
MnFe5(PO4)6 (mp-771656) | 0.2344 | 0.062 | 4 |
Mn2Fe(PO4)3 (mp-776759) | 0.2071 | 0.091 | 4 |
Mn2Cr(PO4)3 (mp-776877) | 0.2317 | 0.088 | 4 |
CrFe2(PO4)3 (mp-777476) | 0.1976 | 1.573 | 4 |
Mn3CoSn2(PO4)6 (mp-765376) | 0.1754 | 0.167 | 5 |
FeNi3Sn2(PO4)6 (mp-853241) | 0.1916 | 0.090 | 5 |
Mn3FeSn2(PO4)6 (mp-776118) | 0.1857 | 0.087 | 5 |
MnCr2Fe3(PO4)6 (mp-776060) | 0.2014 | 1.604 | 5 |
Cr2Fe3Cu(PO4)6 (mp-776010) | 0.2183 | 1.637 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6554 | 0.080 | 6 |
Li4Mn3NbV2(PO4)6 (mp-770640) | 0.6782 | 0.095 | 6 |
Li4MnCr2Fe3(PO4)6 (mp-779026) | 0.6982 | 1.367 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6847 | 0.008 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.6811 | 0.778 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Sn_d P O |
Final Energy/Atom-7.1847 eV |
Corrected Energy-282.2293 eV
-282.2293 eV = -258.6509 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)