Final Magnetic Moment0.993 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.967 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.083 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3Ni2P2(CO7)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 292.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 67.9 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 272.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 203.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 109.5 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 181.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 292.2 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 67.9 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 181.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 109.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 292.2 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 203.7 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 109.5 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 219.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 292.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 292.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 292.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 292.2 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 203.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 181.4 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 277.3 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 277.3 |
BN (mp-984) | <0 0 1> | <1 0 1> | 109.5 |
BN (mp-984) | <1 1 0> | <1 0 0> | 277.3 |
MoS2 (mp-1434) | <1 0 0> | <0 1 1> | 272.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 67.9 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 181.4 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 135.8 |
C (mp-66) | <1 0 0> | <0 1 0> | 203.7 |
C (mp-66) | <1 1 0> | <1 0 1> | 109.5 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 277.3 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 203.7 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 271.5 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 67.9 |
KP(HO2)2 (mp-23959) | <1 0 1> | <0 1 0> | 135.8 |
InSb (mp-20012) | <1 1 0> | <0 1 1> | 181.4 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 233.8 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 271.5 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 1> | 219.0 |
Ga2O3 (mp-886) | <1 1 -1> | <0 0 1> | 233.8 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 109.5 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 292.2 |
CdSe (mp-2691) | <1 1 0> | <1 0 1> | 109.5 |
WS2 (mp-224) | <1 0 0> | <0 1 1> | 90.7 |
WSe2 (mp-1821) | <1 0 1> | <0 1 0> | 203.7 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 0> | 203.7 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 0> | 203.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 203.7 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 0> | 277.3 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 203.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Fe7(PO4)6 (mp-762519) | 0.7491 | 0.272 | 4 |
LiSn10(PO4)7 (mp-765193) | 0.6933 | 0.086 | 4 |
ZnP2W2O9 (mvc-10178) | 0.7370 | 0.308 | 4 |
MnZnPO5 (mvc-3247) | 0.7482 | 0.029 | 4 |
Na3Ni2P2(CO7)2 (mp-768098) | 0.1574 | 0.107 | 5 |
Na3Ni2P2(CO7)2 (mp-775568) | 0.1194 | 0.105 | 5 |
Na3Ni2P2(CO7)2 (mp-775348) | 0.1273 | 0.133 | 5 |
Na3Ni2P2(CO7)2 (mp-769492) | 0.0517 | 0.085 | 5 |
Na3Ni2P2(CO7)2 (mp-767968) | 0.1439 | 0.116 | 5 |
Na5LiCo2P2(CO7)2 (mp-761297) | 0.6893 | 0.013 | 6 |
NaLiMnPCO7 (mp-763833) | 0.6520 | 0.000 | 6 |
Na5LiNi2P2(CO7)2 (mp-770324) | 0.6273 | 0.009 | 6 |
Na2LiFePCO7 (mp-773705) | 0.6626 | 0.138 | 6 |
Na5LiNi2P2(CO7)2 (mp-771060) | 0.7046 | 0.011 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Na_pv Ni_pv P C O |
Final Energy/Atom-6.3099 eV |
Corrected Energy-318.5745 eV
-318.5745 eV = -290.2544 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 8.6560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)