Final Magnetic Moment0.085 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.055 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.524 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi5Cr3(PO4)4 + CrP + Cr2P2O7 + Cr2O3 |
Band Gap0.063 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2CrO4 (mp-764193) | 0.4787 | 0.018 | 3 |
Be(GaO2)2 (mp-676950) | 0.4741 | 0.116 | 3 |
Zn2SiO4 (mp-1020721) | 0.4544 | 0.111 | 3 |
Zn2SiO4 (mp-1020636) | 0.4280 | 0.052 | 3 |
Li2SO4 (mp-4556) | 0.3522 | 0.000 | 3 |
LiCrPO4 (mp-773799) | 0.0517 | 0.067 | 4 |
LiNiPO4 (mp-705448) | 0.1818 | 0.223 | 4 |
LiMnPO4 (mp-585432) | 0.1972 | 0.186 | 4 |
LiFePO4 (mp-585433) | 0.1663 | 0.795 | 4 |
LiMnPO4 (mp-540108) | 0.1933 | 0.737 | 4 |
SiC2 (mp-1019097) | 0.6439 | 0.562 | 2 |
CN2 (mp-1077595) | 0.7413 | 0.691 | 2 |
Li4Ga3Si3IO12 (mp-557112) | 0.6159 | 0.000 | 5 |
Li4Ga3Si3ClO12 (mp-554203) | 0.6564 | 0.000 | 5 |
LiAl3Si9(N7O)2 (mp-695365) | 0.6508 | 0.046 | 5 |
NaBe2BO3F2 (mp-556865) | 0.6490 | 0.006 | 5 |
Li4Ga3Si3BrO12 (mp-556649) | 0.6403 | 0.000 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.5762 | 0.003 | 6 |
C (mp-568410) | 0.6596 | 0.507 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-6.6185 eV |
Corrected Energy-818.4250 eV
-818.4250 eV = -741.2705 eV (uncorrected energy) - 44.9466 eV (MP Anion Correction) - 32.2080 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)