Final Magnetic Moment5.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.238 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi2P2O7 + NbPO5 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 342.2 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 196.6 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 171.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 245.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 245.7 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 198.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 245.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 66.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 318.5 |
Al (mp-134) | <1 1 0> | <0 1 1> | 285.2 |
Al (mp-134) | <1 1 1> | <1 1 0> | 230.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 144.8 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 307.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 231.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 344.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 318.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 228.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 342.2 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 285.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 202.7 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 132.1 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 264.2 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 245.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 66.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 86.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 245.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 202.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 198.2 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 144.8 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 236.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 202.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 231.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 330.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 144.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 57.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 245.7 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 1> | 228.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 260.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 260.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 66.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 144.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 144.8 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 173.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 318.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 285.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 230.3 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 153.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 342.2 |
TiO2 (mp-2657) | <1 1 0> | <1 0 1> | 198.2 |
TiO2 (mp-2657) | <1 1 1> | <1 0 1> | 264.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2P3O10 (mp-540351) | 0.3616 | 0.022 | 3 |
FePO4 (mp-25001) | 0.3568 | 0.017 | 3 |
Co2P3O10 (mp-25658) | 0.3523 | 0.024 | 3 |
Fe2P3O10 (mp-540498) | 0.3504 | 0.039 | 3 |
Ni2P3O10 (mp-25610) | 0.2825 | 0.046 | 3 |
TiNi3(PO4)4 (mp-775517) | 0.1308 | 0.082 | 4 |
VNi3(PO4)4 (mp-775192) | 0.1250 | 0.085 | 4 |
NbCo3(PO4)4 (mp-772014) | 0.1540 | 0.065 | 4 |
Co3Sb(PO4)4 (mp-768012) | 0.1337 | 0.069 | 4 |
TiNi(PO4)2 (mp-774140) | 0.1479 | 0.033 | 4 |
CrO2 (mvc-11581) | 0.7245 | 0.163 | 2 |
VO2 (mp-777469) | 0.7491 | 0.039 | 2 |
Cr5O12 (mp-19575) | 0.7285 | 0.025 | 2 |
VO2 (mvc-6918) | 0.6933 | 0.099 | 2 |
MoO2 (mvc-6944) | 0.6341 | 0.289 | 2 |
MnFeCo(PO4)3 (mp-764410) | 0.1977 | 0.026 | 5 |
MnFeCo(PO4)3 (mp-764392) | 0.2242 | 0.027 | 5 |
MnFeCo(PO4)3 (mp-763496) | 0.2208 | 0.026 | 5 |
MnFeCo(PO4)3 (mp-764415) | 0.2008 | 0.028 | 5 |
MnFeCo(PO4)3 (mp-763446) | 0.2049 | 0.026 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6755 | 0.084 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.4914 | 0.002 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6276 | 0.020 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5809 | 0.045 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.6858 | 0.013 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6474 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Nb_pv Ni_pv P O |
Final Energy/Atom-6.8384 eV |
Corrected Energy-181.8502 eV
-181.8502 eV = -164.1215 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 6.4920 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)