material

HfO2

ID:

mp-775757

DOI:

10.17188/1303484


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-4.020 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.010 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
HfO2
Band Gap
4.017 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pbca [61]
Hall
-P 2ac 2ab
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
No elastic tensor calculated for this material, so elastic energies not avaialable. Sorting by MCIA instead.
substrate material substrate orientation film orientation MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 247.1
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 137.3
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 302.1
LaAlO3 (mp-2920) <1 1 0> <0 0 1> 247.1
AlN (mp-661) <0 0 1> <1 0 0> 269.3
AlN (mp-661) <1 0 0> <0 1 0> 158.2
AlN (mp-661) <1 0 1> <0 1 1> 178.3
AlN (mp-661) <1 1 0> <1 0 0> 53.9
AlN (mp-661) <1 1 1> <0 1 0> 316.3
CeO2 (mp-20194) <1 0 0> <0 0 1> 247.1
GaAs (mp-2534) <1 0 0> <0 1 0> 263.6
GaAs (mp-2534) <1 1 0> <1 0 1> 181.4
GaN (mp-804) <0 0 1> <1 0 1> 181.4
GaN (mp-804) <1 0 0> <0 0 1> 82.4
GaN (mp-804) <1 1 0> <0 1 1> 59.4
GaN (mp-804) <1 1 1> <1 1 1> 240.6
SiO2 (mp-6930) <0 0 1> <0 1 0> 263.6
SiO2 (mp-6930) <1 0 0> <1 1 0> 226.1
SiO2 (mp-6930) <1 0 1> <1 1 1> 240.6
SiO2 (mp-6930) <1 1 0> <1 0 0> 323.2
SiO2 (mp-6930) <1 1 1> <1 1 1> 160.4
DyScO3 (mp-31120) <0 0 1> <1 0 1> 60.5
DyScO3 (mp-31120) <0 1 0> <0 0 1> 82.4
DyScO3 (mp-31120) <1 0 0> <0 1 1> 178.3
DyScO3 (mp-31120) <1 1 0> <0 0 1> 247.1
DyScO3 (mp-31120) <1 1 1> <1 0 0> 269.3
ZnSe (mp-1190) <1 0 0> <0 1 0> 263.6
ZnSe (mp-1190) <1 1 0> <1 0 1> 181.4
KTaO3 (mp-3614) <1 0 0> <0 1 0> 263.6
KTaO3 (mp-3614) <1 1 0> <1 0 1> 181.4
KTaO3 (mp-3614) <1 1 1> <1 1 0> 226.1
CdS (mp-672) <0 0 1> <0 0 1> 137.3
CdS (mp-672) <1 0 0> <1 0 0> 269.3
CdS (mp-672) <1 0 1> <0 1 1> 297.2
CdS (mp-672) <1 1 0> <1 1 0> 150.7
LiF (mp-1138) <1 0 0> <1 1 0> 150.7
LiF (mp-1138) <1 1 0> <0 1 0> 210.9
Te2W (mp-22693) <0 0 1> <0 0 1> 247.1
Te2W (mp-22693) <1 1 0> <1 1 0> 226.1
Te2Mo (mp-602) <0 0 1> <0 1 1> 178.3
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 302.1
GaSe (mp-1943) <0 0 1> <0 0 1> 192.2
GaSe (mp-1943) <1 0 1> <0 1 0> 210.9
BN (mp-984) <0 0 1> <0 1 0> 263.6
BN (mp-984) <1 0 0> <0 1 0> 158.2
BN (mp-984) <1 0 1> <0 1 0> 158.2
BN (mp-984) <1 1 0> <0 0 1> 164.8
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 137.3
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 219.7
YVO4 (mp-19133) <0 0 1> <1 1 1> 160.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
326 105 177 0 0 0
105 379 155 0 0 0
177 155 381 0 0 0
0 0 0 131 0 0
0 0 0 0 100 0
0 0 0 0 0 75
Compliance Tensor Sij (10-12Pa-1)
4.2 -0.4 -1.8 0 0 0
-0.4 3.2 -1.1 0 0 0
-1.8 -1.1 3.9 0 0 0
0 0 0 7.6 0 0
0 0 0 0 10 0
0 0 0 0 0 13.3
Shear Modulus GV
104 GPa
Bulk Modulus KV
218 GPa
Shear Modulus GR
99 GPa
Bulk Modulus KR
214 GPa
Shear Modulus GVRH
102 GPa
Bulk Modulus KVRH
216 GPa
Elastic Anisotropy
0.28
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TaNO (mp-4165) 0.2887 0.000 3
CeZr11O24 (mp-752706) 0.2811 0.017 3
VOF (mp-768037) 0.3028 0.012 3
ScOF (mp-4661) 0.3037 0.000 3
NbNO (mp-7596) 0.3069 0.000 3
ZrO2 (mp-2858) 0.1907 0.000 2
HfO2 (mp-352) 0.2135 0.000 2
ZrO2 (mp-776404) 0.0641 0.009 2
NdO2 (mp-755820) 0.3587 0.169 2
CeSe2 (mp-1080303) 0.3335 0.024 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

To confirm the nature of the released species we combined IR, NMR, and X-ray fluorescence (XRF) analysis. Upon addition of Am to HfO2 NCs, the expected carboxylic acid band at 1720cm1 is absent in t [...]
High purity HfO2 (99.9% purity) 5inch sputtering target supplied by M/s Semiconductor technology was used to deposit the thin films in MRC rf sputtering machine. The films were deposited on p- type 1 [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition HfO2.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv O
Final Energy/Atom
-10.1699 eV
Corrected Energy
-255.3139 eV
-255.3139 eV = -244.0772 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by