Final Magnetic Moment1.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.900 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.082 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAl2O3 + V2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 79.6 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 309.2 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 141.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 146.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 238.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 309.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 141.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 309.2 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 238.7 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 135.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 146.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 185.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 291.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 238.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 238.7 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 282.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 282.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 220.9 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 132.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 141.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 282.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 70.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 265.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 132.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 44.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 141.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 309.2 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 203.3 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 152.5 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 135.4 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 50.8 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 88.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 328.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 282.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 212.2 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 225.7 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 220.9 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 106.0 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 282.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 238.7 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 132.5 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 282.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 88.3 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 176.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 344.8 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 88.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 146.1 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 282.6 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 70.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 309.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaBiO3 (mvc-3850) | 0.1829 | 0.016 | 3 |
LaErO3 (mp-7538) | 0.1903 | 0.027 | 3 |
CaPbO3 (mp-20079) | 0.2034 | 0.002 | 3 |
LaYO3 (mp-10429) | 0.2108 | 0.039 | 3 |
LaTmO3 (mp-13374) | 0.2012 | 0.020 | 3 |
Mg2VIrO6 (mvc-5771) | 0.2548 | 0.144 | 4 |
Mg2TiIrO6 (mvc-5583) | 0.2561 | 0.126 | 4 |
PrMg(SnO3)2 (mvc-9297) | 0.2521 | 0.229 | 4 |
CaHo(WO3)2 (mvc-10339) | 0.2624 | 0.137 | 4 |
CaPr(SnO3)2 (mvc-9344) | 0.2523 | 0.133 | 4 |
CoTe2 (mp-1077715) | 0.6387 | 0.020 | 2 |
Te2Ir (mp-569322) | 0.6161 | 0.012 | 2 |
Al2O3 (mp-642363) | 0.5496 | 0.280 | 2 |
Te2Ir (mp-569388) | 0.6367 | 0.000 | 2 |
Te2Ir (mp-1551) | 0.6144 | 0.006 | 2 |
LaMgFeSnO6 (mvc-9082) | 0.3268 | 0.293 | 5 |
LaMgCrMoO6 (mvc-9867) | 0.3225 | 0.712 | 5 |
LaMgCrSbO6 (mvc-9859) | 0.3347 | 0.842 | 5 |
LaMgCrBiO6 (mvc-9861) | 0.3558 | 0.793 | 5 |
LaMgCrSnO6 (mvc-9925) | 0.3108 | 0.773 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Al V_pv O |
Final Energy/Atom-7.6766 eV |
Corrected Energy-168.6871 eV
-168.6871 eV = -153.5316 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)