Final Magnetic Moment23.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFerri |
Formation Energy / Atom-1.753 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.086 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeSbO4 + O2 + MnO2 + Fe2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 166.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 329.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 164.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 274.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 244.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 122.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 109.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 244.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 122.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 329.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 287.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 244.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 164.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 164.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 329.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 244.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 166.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 244.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 183.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 305.2 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 249.1 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 274.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 122.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 305.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 274.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 274.4 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 329.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 164.7 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 244.1 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 305.2 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 274.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 274.4 |
C (mp-66) | <1 0 0> | <0 0 1> | 305.2 |
C (mp-66) | <1 1 0> | <0 0 1> | 183.1 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 164.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 244.1 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 329.3 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 287.8 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 329.3 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 244.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 221.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 1> | 249.1 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 183.1 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 274.4 |
Au (mp-81) | <1 0 0> | <1 0 0> | 274.4 |
C (mp-48) | <0 0 1> | <0 1 1> | 227.4 |
WSe2 (mp-1821) | <0 0 1> | <1 0 1> | 249.1 |
WSe2 (mp-1821) | <1 0 1> | <0 0 1> | 305.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3Ni3(TeO8)2 (mp-771860) | 0.1500 | 0.051 | 4 |
Ti3Fe3(SbO8)2 (mp-764329) | 0.1991 | 0.122 | 4 |
Fe3Co3(SbO8)2 (mp-761701) | 0.2116 | 0.113 | 4 |
Ti3Mn3(SbO8)2 (mp-763292) | 0.2063 | 0.084 | 4 |
Mn3Nb2Fe3O16 (mp-775243) | 0.2111 | 0.093 | 4 |
TiO2 (mp-756587) | 0.3092 | 0.111 | 2 |
TiO2 (mp-766454) | 0.2970 | 0.059 | 2 |
MnO2 (mp-715581) | 0.3212 | 0.020 | 2 |
MnO2 (mp-644514) | 0.3201 | 0.019 | 2 |
MnO2 (mp-773240) | 0.2976 | 0.029 | 2 |
MnCr3O8 (mp-764180) | 0.2454 | 0.091 | 3 |
Mn3VO8 (mp-771584) | 0.2687 | 0.065 | 3 |
Mn3Cr5O16 (mp-773259) | 0.2335 | 0.077 | 3 |
Ti5Mn3O16 (mp-776807) | 0.2669 | 0.095 | 3 |
Ti3V5O16 (mp-776923) | 0.2187 | 0.107 | 3 |
LaMnZnFeO6 (mvc-8951) | 0.7436 | 0.082 | 5 |
LaZnCrWO6 (mvc-9890) | 0.6770 | 0.167 | 5 |
SrLaMnRuO6 (mp-39239) | 0.6532 | 0.000 | 5 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.7022 | 0.058 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points32 |
U ValuesMn: 3.9 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Mn_pv Fe_pv Sb O |
Final Energy/Atom-6.5696 eV |
Corrected Energy-182.1476 eV
-182.1476 eV = -157.6694 eV (uncorrected energy) - 13.2416 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)