Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-3.480 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiO2 |
Band Gap2.084 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 276.0 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 282.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 307.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 205.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 51.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 83.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 179.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 154.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 87.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 230.9 |
GaAs (mp-2534) | <1 1 1> | <0 1 1> | 220.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 166.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 128.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 307.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 230.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 128.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 230.9 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 87.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 154.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 359.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 128.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 154.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 282.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 205.3 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 207.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 83.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 256.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 282.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 205.3 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 174.3 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 216.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 179.6 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 230.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 87.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 166.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 230.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 294.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 333.6 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 179.6 |
ZnSe (mp-1190) | <1 1 1> | <0 1 1> | 220.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 282.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 216.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 282.3 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 261.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 216.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 333.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 205.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 333.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 307.9 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 216.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YTa(WO4)2 (mvc-765) | 0.2968 | 0.091 | 4 |
YRe(WO4)2 (mvc-853) | 0.2719 | 0.154 | 4 |
NaMnCrF6 (mp-554827) | 0.2508 | 0.000 | 4 |
LiMnFeF6 (mp-555001) | 0.2828 | 0.000 | 4 |
LiMnGaF6 (mp-558902) | 0.2613 | 0.000 | 4 |
TiO2 (mvc-6590) | 0.4130 | 0.038 | 2 |
SnO2 (mp-555487) | 0.3145 | 0.012 | 2 |
SiO2 (mp-32667) | 0.2942 | 0.243 | 2 |
HfO2 (mp-776097) | 0.2175 | 0.028 | 2 |
ZrO2 (mp-775980) | 0.2125 | 0.052 | 2 |
LiCu2F6 (mp-863372) | 0.2695 | 0.022 | 3 |
Lu2TeO6 (mp-755515) | 0.2729 | 0.000 | 3 |
LiVF4 (mp-767647) | 0.2394 | 0.012 | 3 |
Fe3(OF2)2 (mp-763816) | 0.2683 | 0.083 | 3 |
Fe6O5F7 (mp-773740) | 0.2687 | 0.094 | 3 |
SrLaMnRuO6 (mp-39239) | 0.6994 | 0.000 | 5 |
Li4MnSn(WO6)2 (mp-775961) | 0.7236 | 0.055 | 5 |
Li4MnCr(WO6)2 (mp-761370) | 0.6904 | 0.068 | 5 |
Li7Zr3Nb(TeO6)4 (mp-695434) | 0.6821 | 0.016 | 5 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.6339 | 0.058 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points6 |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv O |
Final Energy/Atom-8.9344 eV |
Corrected Energy-338.4924 eV
-338.4924 eV = -321.6375 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)