Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.896 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.233 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa4VO4 + NaVO2 + Na |
Band Gap0.383 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFddd [70] |
HallF 2 2 1d |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 282.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 339.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 282.6 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 134.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 244.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 282.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 169.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 113.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 169.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 282.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 282.6 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 282.6 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 198.8 |
Al (mp-134) | <1 0 0> | <0 1 0> | 244.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 282.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 122.1 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 122.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 282.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 226.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 282.6 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 190.5 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 339.2 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 198.8 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 282.6 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 244.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 282.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 226.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 282.6 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 244.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 339.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 339.2 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 190.5 |
Au (mp-81) | <1 0 0> | <0 0 1> | 282.6 |
Au (mp-81) | <1 1 0> | <0 1 0> | 122.1 |
Au (mp-81) | <1 1 1> | <0 1 0> | 122.1 |
C (mp-48) | <0 0 1> | <0 0 1> | 282.6 |
SiC (mp-11714) | <0 0 1> | <1 0 1> | 198.8 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 190.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 282.6 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 282.6 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 339.2 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 190.5 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 134.6 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 0> | 122.1 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 339.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 282.6 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 282.6 |
CdWO4 (mp-19387) | <1 0 1> | <0 1 1> | 134.6 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 339.2 |
MgF2 (mp-1249) | <1 1 0> | <0 1 0> | 122.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2FeO3 (mp-764467) | 0.6620 | 0.259 | 3 |
Na6Sn2O7 (mp-777814) | 0.4986 | 0.074 | 3 |
Li3(FeO3)2 (mp-763576) | 0.6722 | 0.066 | 3 |
Li3Mn4O8 (mp-1003769) | 0.5925 | 0.064 | 3 |
Na4Mn2O5 (mp-18869) | 0.4953 | 0.000 | 3 |
Li6Mn2O5F2 (mp-767601) | 0.6734 | 0.180 | 4 |
Li3Mn3CrO8 (mp-764036) | 0.6888 | 0.266 | 4 |
Li6Mn5Ni3O16 (mp-763980) | 0.6773 | 0.080 | 4 |
Li6Co3Ni5O16 (mp-763964) | 0.6656 | 0.070 | 4 |
Li4FeOF5 (mp-779064) | 0.6533 | 0.093 | 4 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.6978 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv V_pv O |
Final Energy/Atom-5.6486 eV |
Corrected Energy-137.9391 eV
Uncorrected energy = -124.2691 eV
Composition-based energy adjustment (-0.687 eV/atom x 10.0 atoms) = -6.8700 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -137.9391 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)