Final Magnetic Moment14.987 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.846 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnNbO4 + Li2Ti3MnO8 |
Band Gap1.039 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 240.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 323.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 323.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 323.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 323.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 323.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 300.4 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 194.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 60.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 258.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 194.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 240.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 323.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 323.4 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 180.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 180.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 129.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 194.0 |
C (mp-66) | <1 1 0> | <1 0 0> | 180.3 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 323.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 258.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 258.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 258.7 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 267.3 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 240.3 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 258.7 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 212.1 |
SiC (mp-11714) | <0 0 1> | <1 0 1> | 267.3 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 60.1 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 300.4 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 1> | 138.5 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 258.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 300.4 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 267.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 258.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 129.4 |
Ga2O3 (mp-886) | <1 1 -1> | <1 1 0> | 243.8 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 300.4 |
Si (mp-149) | <1 1 0> | <0 0 1> | 323.4 |
Au (mp-81) | <1 1 0> | <1 0 0> | 300.4 |
Au (mp-81) | <1 1 1> | <1 0 0> | 60.1 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 258.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 323.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 212.1 |
C (mp-48) | <1 0 0> | <0 1 1> | 248.5 |
WSe2 (mp-1821) | <1 0 1> | <1 0 0> | 300.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 258.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 258.7 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 323.4 |
ZrO2 (mp-2858) | <1 1 0> | <0 0 1> | 323.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li7W5O16 (mp-771579) | 0.2889 | 0.031 | 3 |
Ca(CoO2)2 (mvc-5503) | 0.3186 | 0.266 | 3 |
Ca(CoO2)2 (mvc-5217) | 0.3265 | 0.282 | 3 |
Ca(WO2)2 (mvc-10486) | 0.3621 | 0.499 | 3 |
Mg(SnO2)2 (mvc-9750) | 0.3559 | 0.242 | 3 |
Li7Mn3(WO8)2 (mp-771587) | 0.1513 | 0.107 | 4 |
Li7Cr3(WO8)2 (mp-771537) | 0.1958 | 0.057 | 4 |
Li7Fe3(WO8)2 (mp-771510) | 0.1809 | 0.090 | 4 |
Li4Ti5Ni3O16 (mp-771465) | 0.2103 | 0.181 | 4 |
Li4V5Co3O16 (mp-776751) | 0.1980 | 0.327 | 4 |
Si3N4 (mp-641539) | 0.4967 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4616 | 0.208 | 2 |
Mn3N4 (mp-1080204) | 0.5157 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.5264 | 0.227 | 2 |
Re3N4 (mp-1080201) | 0.5498 | 0.110 | 2 |
Li4Ti3Nb2Co3O16 (mp-776800) | 0.1381 | 0.023 | 5 |
Li4Nb2V3Co3O16 (mp-775090) | 0.1478 | 0.116 | 5 |
Li4V2Cr3Ni3O16 (mp-769730) | 0.1446 | 0.247 | 5 |
Li4Ti3Nb2Fe3O16 (mp-775999) | 0.1153 | 0.018 | 5 |
Li4V2Co3Ni3O16 (mp-763125) | 0.1489 | 0.119 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6746 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.6850 | 0.599 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6816 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6871 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6801 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Mn_pv Nb_pv O |
Final Energy/Atom-7.9134 eV |
Corrected Energy-237.8537 eV
-237.8537 eV = -221.5745 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 5.0426 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)