Final Magnetic Moment0.071 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.516 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.130 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVP + VPO4 |
Band Gap2.395 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP41 [76] |
HallP 4w |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 127.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 255.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 170.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 340.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 154.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 298.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 213.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 340.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 213.1 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 213.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 85.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 213.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 42.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 213.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 213.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 298.3 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 42.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 340.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 213.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 298.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 298.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 170.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 340.9 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 213.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 170.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 340.9 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 42.6 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 298.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 340.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 213.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 340.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 340.9 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 298.3 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 154.2 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 298.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 213.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 42.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 170.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 255.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 298.3 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 340.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 298.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 85.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 127.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 213.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 213.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 213.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 170.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 298.3 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 42.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3(P2O7)2 (mp-706469) | 0.4883 | 0.059 | 3 |
NaPO3 (mp-558192) | 0.4883 | 0.006 | 3 |
Sn2P2O7 (mp-753979) | 0.4875 | 0.049 | 3 |
Hg2P2O7 (mp-28455) | 0.3994 | 0.000 | 3 |
Mn2P3O10 (mp-31981) | 0.4678 | 0.030 | 3 |
MgFeP2O7 (mvc-5721) | 0.4213 | 0.022 | 4 |
ZnFeP2O7 (mvc-5718) | 0.4147 | 0.021 | 4 |
MgNiP2O7 (mvc-5642) | 0.4071 | 0.026 | 4 |
ZnCoP2O7 (mvc-5639) | 0.4205 | 0.024 | 4 |
MgCoP2O7 (mvc-5586) | 0.4217 | 0.035 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.6129 | 0.087 | 5 |
KCu3Ag(MoO4)4 (mp-699550) | 0.6019 | 0.019 | 5 |
Li2Mn2Fe(PO4)3 (mp-776051) | 0.6485 | 0.094 | 5 |
LiAg2P3(HO5)2 (mp-695951) | 0.6016 | 0.020 | 5 |
SrVZnP2O9 (mp-555402) | 0.6379 | 0.007 | 5 |
Li4Mn3NbV2(PO4)6 (mp-770640) | 0.7234 | 0.095 | 6 |
Li4Mn2VNi3(PO4)6 (mp-770417) | 0.7215 | 0.075 | 6 |
Li4Mn3NbCr2(PO4)6 (mp-776566) | 0.6839 | 0.102 | 6 |
Li4TiMn3Cr2(PO4)6 (mp-778261) | 0.6909 | 0.081 | 6 |
Li4Mn2Fe3Sb(PO4)6 (mp-776752) | 0.7020 | 3.420 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv P O |
Final Energy/Atom-7.5242 eV |
Corrected Energy-728.3730 eV
-728.3730 eV = -662.1328 eV (uncorrected energy) - 39.3282 eV (MP Anion Correction) - 26.9120 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)