Final Magnetic Moment18.304 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.317 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + CrPO4 + Cu2PO5 + Cr(PO3)3 + MnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 321.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 321.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 193.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 193.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 175.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 257.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 175.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 64.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 193.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 128.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 193.0 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 193.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 64.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 321.6 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 193.0 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 257.3 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 257.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 193.0 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 64.3 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 257.3 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 193.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 175.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 321.6 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 321.6 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 193.0 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 64.3 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 64.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 257.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 321.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 175.3 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 175.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 193.0 |
C (mp-66) | <1 1 1> | <1 0 0> | 175.3 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 321.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 321.6 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 257.3 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 257.3 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 257.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 64.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 193.0 |
C (mp-48) | <0 0 1> | <0 0 1> | 257.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 257.3 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 257.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 193.0 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 257.3 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 193.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.3567 | 0.344 | 3 |
VPO4 (mp-861584) | 0.2693 | 0.079 | 3 |
FePO4 (mp-773675) | 0.1657 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.1905 | 0.077 | 3 |
VPO4 (mp-32453) | 0.3537 | 0.112 | 3 |
Mn2Cr(PO4)3 (mp-776877) | 0.1005 | 0.088 | 4 |
Fe5Ni(PO4)6 (mp-770337) | 0.1193 | 0.064 | 4 |
Fe5Cu(PO4)6 (mp-771903) | 0.1014 | 0.062 | 4 |
MnCr(PO4)2 (mp-780896) | 0.1201 | 0.083 | 4 |
CrFe5(PO4)6 (mp-771182) | 0.1193 | 1.150 | 4 |
VO2 (mvc-6918) | 0.6874 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6272 | 0.281 | 2 |
Mn3VCr2(PO4)6 (mp-765402) | 0.1213 | 0.082 | 5 |
Fe3Co2Cu(PO4)6 (mp-762161) | 0.0751 | 0.084 | 5 |
MnCr2Ni3(PO4)6 (mp-777895) | 0.1062 | 0.098 | 5 |
Mn3Cr2Ni(PO4)6 (mp-776047) | 0.0532 | 0.079 | 5 |
Cr2Fe3Cu(PO4)6 (mp-776010) | 0.1138 | 1.637 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5836 | 0.080 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6109 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.5181 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.6154 | 0.015 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.6237 | 0.778 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Mn_pv Cr_pv Cu_pv P O |
Final Energy/Atom-7.2111 eV |
Corrected Energy-285.5221 eV
-285.5221 eV = -259.5986 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 9.0686 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)