Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.369 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg3O4 + O2 + Au2O3 |
Band Gap0.242 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 212.3 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 183.9 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 212.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 106.2 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 183.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 212.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 183.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 212.3 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 212.3 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 183.9 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 183.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 150.1 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 183.9 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 150.1 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 183.9 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 212.3 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 106.2 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 150.1 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 183.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
192 | 93 | 93 | 0 | 0 | 0 |
93 | 192 | 93 | 0 | 0 | 0 |
93 | 93 | 192 | 0 | 0 | 0 |
0 | 0 | 0 | 61 | 0 | 0 |
0 | 0 | 0 | 0 | 61 | 0 |
0 | 0 | 0 | 0 | 0 | 61 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
7.6 | -2.5 | -2.5 | 0 | 0 | 0 |
-2.5 | 7.6 | -2.5 | 0 | 0 | 0 |
-2.5 | -2.5 | 7.6 | 0 | 0 | 0 |
0 | 0 | 0 | 16.5 | 0 | 0 |
0 | 0 | 0 | 0 | 16.5 | 0 |
0 | 0 | 0 | 0 | 0 | 16.5 |
Shear Modulus GV56 GPa |
Bulk Modulus KV126 GPa |
Shear Modulus GR56 GPa |
Bulk Modulus KR126 GPa |
Shear Modulus GVRH56 GPa |
Bulk Modulus KVRH126 GPa |
Elastic Anisotropy0.05 |
Poisson's Ratio0.31 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points8 |
U Values-- |
PseudopotentialsVASP PAW: Ag Au O |
Final Energy/Atom-4.1305 eV |
Corrected Energy-91.0379 eV
-91.0379 eV = -82.6104 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)