Final Magnetic Moment6.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.818 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.488 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 262.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 157.2 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 252.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 325.8 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 139.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 262.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 140.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 232.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 314.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 232.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 232.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 197.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 262.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 325.8 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 197.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 252.4 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 329.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 209.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 232.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 262.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 262.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 262.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 140.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 210.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 280.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 139.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 209.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 252.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 263.3 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 252.4 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 210.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 262.0 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 263.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 262.0 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 65.8 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 197.5 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 168.3 |
Te2W (mp-22693) | <1 1 1> | <1 0 0> | 232.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 52.4 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 65.8 |
YVO4 (mp-19133) | <1 1 1> | <1 1 1> | 84.1 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 232.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 46.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 70.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 209.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 262.0 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 325.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 262.0 |
GaSe (mp-1943) | <1 1 1> | <1 0 0> | 232.7 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 232.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YAsO4 (mp-8058) | 0.0595 | 0.000 | 3 |
DyAsO4 (mp-5632) | 0.0658 | 0.000 | 3 |
TbAsO4 (mp-3248) | 0.0450 | 0.000 | 3 |
EuAsO4 (mp-13576) | 0.0804 | 0.000 | 3 |
SmAsO4 (mp-12929) | 0.0395 | 0.000 | 3 |
CaU(PO4)2 (mp-9360) | 0.4958 | 0.000 | 4 |
Cr2AgBiO8 (mp-565669) | 0.5554 | 0.011 | 4 |
Er2SiSO4 (mp-555990) | 0.5688 | 0.020 | 4 |
PrTl(MoO4)2 (mp-19579) | 0.5728 | 0.006 | 4 |
Ca2BAsO8 (mp-1095596) | 0.5383 | 0.242 | 4 |
TlCl2 (mp-27205) | 0.5650 | 0.000 | 2 |
TlBr2 (mp-27398) | 0.4804 | 0.000 | 2 |
InI2 (mp-29312) | 0.4762 | 0.000 | 2 |
InBr2 (mp-568108) | 0.4762 | 0.000 | 2 |
GaCl2 (mp-568848) | 0.4992 | 0.000 | 2 |
DyZr9Si9PO40 (mp-686636) | 0.3571 | 0.011 | 5 |
YZr5Si5PO24 (mp-532768) | 0.3791 | 0.014 | 5 |
KCaNd(PO4)2 (mp-676934) | 0.5324 | 0.000 | 5 |
YbZr7Si7PO32 (mp-690946) | 0.4075 | 0.019 | 5 |
ErZr11Si11PO48 (mp-690951) | 0.3310 | 0.008 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Gd As O |
Final Energy/Atom-8.7706 eV |
Corrected Energy-110.7429 eV
Uncorrected energy = -105.2469 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -110.7429 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)