Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.250 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.097 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3VO4 + FeO + LiVO2 |
Band Gap0.008 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 -1> | 287.7 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 198.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 105.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 236.7 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 309.7 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 116.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 116.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 -1> | 348.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 158.4 |
LiF (mp-1138) | <1 0 0> | <0 1 -1> | 193.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 189.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 236.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 -1> | 193.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 189.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 274.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 -1> | 271.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 198.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 -1> | 154.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 184.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 -1> | 154.9 |
YVO4 (mp-19133) | <1 1 0> | <1 -1 1> | 265.3 |
GaN (mp-804) | <0 0 1> | <1 -1 0> | 143.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 131.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 210.4 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 116.1 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 116.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 131.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 276.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 237.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 184.1 |
KCl (mp-23193) | <1 1 1> | <1 0 -1> | 284.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 162.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 162.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 162.6 |
Te2Mo (mp-602) | <1 1 1> | <1 -1 -1> | 279.8 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 172.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 189.4 |
Ag (mp-124) | <1 1 1> | <1 0 -1> | 122.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 184.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 348.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 315.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 189.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 277.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 -1> | 193.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 0> | 143.3 |
InAs (mp-20305) | <1 0 0> | <1 -1 0> | 334.4 |
InAs (mp-20305) | <1 1 0> | <0 1 -1> | 271.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 158.4 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 193.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 189.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2BiO3 (mp-780656) | 0.2437 | 0.001 | 3 |
LiMnO2 (mp-772021) | 0.2163 | 0.050 | 3 |
Li7Mn5O12 (mp-771616) | 0.2311 | 0.022 | 3 |
Na2Ni3O5 (mp-765675) | 0.2523 | 0.027 | 3 |
Li7Ni5O12 (mp-771927) | 0.2388 | 0.036 | 3 |
Li9Si2Ni5O16 (mp-859799) | 0.2433 | 0.042 | 4 |
Li5Mn3(SbO5)2 (mp-771439) | 0.2296 | 0.066 | 4 |
Li5Cr2Fe3O10 (mp-765750) | 0.2342 | 1.245 | 4 |
Li3SiNiO5 (mp-772067) | 0.2434 | 0.069 | 4 |
Li2VO2F (mp-763177) | 0.2380 | 0.095 | 4 |
Te2Au (mp-1662) | 0.4549 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3558 | 0.000 | 2 |
TiS (mp-557762) | 0.5343 | 0.139 | 2 |
BaO (mp-776658) | 0.4225 | 0.019 | 2 |
Te2Au (mp-567525) | 0.3897 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.3932 | 0.005 | 5 |
Na (mp-999501) | 0.7351 | 0.116 | 1 |
Sb (mp-632286) | 0.7314 | 0.059 | 1 |
Bi (mp-567379) | 0.7453 | 0.062 | 1 |
Te (mp-570459) | 0.6596 | 0.044 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv O |
Final Energy/Atom-6.5344 eV |
Corrected Energy-148.2229 eV
-148.2229 eV = -130.6880 eV (uncorrected energy) - 10.5120 eV (MP Advanced Correction) - 7.0229 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)