Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.146 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.053 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiO2 + TiN + N2 |
Band Gap1.051 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 220.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 254.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 191.1 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 254.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 254.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 254.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 127.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 127.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 191.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 -1> | 270.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 127.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 156.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 191.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 254.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 191.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 318.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 318.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 220.6 |
TePb (mp-19717) | <1 0 0> | <1 1 -1> | 90.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 191.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 191.1 |
YVO4 (mp-19133) | <1 0 1> | <1 1 -1> | 270.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 191.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 318.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 254.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 254.9 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 220.6 |
CdTe (mp-406) | <1 0 0> | <1 1 -1> | 90.1 |
TeO2 (mp-2125) | <0 1 1> | <1 1 0> | 220.6 |
SiC (mp-7631) | <1 1 0> | <1 0 0> | 254.9 |
MgO (mp-1265) | <1 0 0> | <1 1 -1> | 90.1 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 254.9 |
C (mp-66) | <1 1 1> | <1 1 1> | 156.0 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 220.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 254.9 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 254.9 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 127.4 |
GaP (mp-2490) | <1 1 1> | <1 1 1> | 156.0 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 191.1 |
Al (mp-134) | <1 1 0> | <1 0 0> | 254.9 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 191.1 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 191.1 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 254.9 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 254.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 191.1 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 318.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 191.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 -1> | 270.2 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 254.9 |
PbS (mp-21276) | <1 0 0> | <1 1 -1> | 180.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ti2N2O (mp-776361) | 0.0866 | 0.055 | 3 |
Ti2N2O (mp-776336) | 0.0939 | 0.058 | 3 |
Ti2N2O (mp-776334) | 0.0885 | 0.059 | 3 |
Ti2N2O (mp-849331) | 0.0776 | 0.056 | 3 |
Ti2N2O (mp-776313) | 0.0808 | 0.058 | 3 |
LiMn7(O3F)3 (mp-765039) | 0.3941 | 0.089 | 4 |
Li3Mn5OF11 (mp-767196) | 0.4337 | 0.062 | 4 |
Li3Ni5OF11 (mp-766724) | 0.4207 | 0.055 | 4 |
Li2Fe4OF8 (mp-849951) | 0.4402 | 0.057 | 4 |
Li4Fe2OF8 (mp-776724) | 0.4249 | 0.043 | 4 |
Sr3N2 (mp-986716) | 0.3044 | 0.031 | 2 |
Fe2O3 (mp-715572) | 0.2702 | 0.116 | 2 |
Cr3N2 (mp-1097796) | 0.2727 | 0.114 | 2 |
Cr3N2 (mp-1014318) | 0.2778 | 0.114 | 2 |
Cr2O3 (mp-776873) | 0.3066 | 0.042 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.6069 | 0.083 | 5 |
Li4VFe(TeO6)2 (mp-761819) | 0.6973 | 0.060 | 5 |
Li4MnV2WO12 (mp-773239) | 0.6838 | 0.089 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.6815 | 0.056 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.6669 | 0.104 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ti_pv N O |
Final Energy/Atom-9.3338 eV |
Corrected Energy-378.9721 eV
-378.9721 eV = -373.3538 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)