Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.367 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.184 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToW2N3 + N2 |
Band Gap1.555 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 323.5 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 161.3 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 115.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 325.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 325.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 325.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 323.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 323.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 275.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 258.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 323.5 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 161.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 260.2 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 115.8 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 91.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 260.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 124.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 258.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 161.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 323.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 323.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 323.5 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 275.2 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 265.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 275.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 161.3 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 194.1 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 275.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 194.1 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 325.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 323.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 323.5 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 231.6 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 91.7 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 161.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 323.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 194.1 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 129.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 323.5 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 129.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 64.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 194.1 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 130.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 194.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 258.8 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 258.8 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 325.2 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 -1> | 115.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 1> | 161.3 |
C (mp-66) | <1 0 0> | <1 0 -1> | 115.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoPO4 (mp-851068) | 0.5644 | 0.025 | 3 |
BeCrO4 (mp-770887) | 0.5234 | 0.011 | 3 |
NiPO4 (mp-705637) | 0.5673 | 0.537 | 3 |
PNO (mp-36779) | 0.5715 | 0.015 | 3 |
NiPO4 (mp-697731) | 0.6282 | 0.151 | 3 |
Rb2Al2Si3O10 (mp-975622) | 0.5976 | 0.009 | 4 |
CsSi3HO7 (mp-758180) | 0.6455 | 0.002 | 4 |
K2Be(Si2O5)2 (mp-557802) | 0.6112 | 0.000 | 4 |
K2Zn(Si2O5)2 (mp-555568) | 0.6571 | 0.000 | 4 |
K2Al2Si3O10 (mp-1019744) | 0.5343 | 0.018 | 4 |
SiO2 (mp-560131) | 0.3158 | 0.092 | 2 |
SiO2 (mp-560152) | 0.2465 | 0.098 | 2 |
CeSe2 (mp-1080370) | 0.2615 | 0.503 | 2 |
SiO2 (mp-557134) | 0.3373 | 0.085 | 2 |
CrN2 (mp-1096890) | 0.2993 | 0.461 | 2 |
RbB2P2HO9 (mp-758281) | 0.6883 | 0.000 | 5 |
RbZnB(PO4)2 (mp-557658) | 0.6695 | 0.000 | 5 |
CsZnB(PO4)2 (mp-560244) | 0.6693 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: W_pv N |
Final Energy/Atom-9.9878 eV |
Corrected Energy-359.5600 eV
-359.5600 eV = -359.5600 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)