Final Magnetic Moment0.908 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.642 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg2O + AgO + IrO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4122 [91] |
HallP 4w 2c |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 245.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 275.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 306.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 306.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 247.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 275.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 61.4 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 205.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 260.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 220.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 245.5 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 173.6 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 247.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 275.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 184.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 220.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 220.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 220.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 165.2 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 247.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 245.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 306.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 330.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 245.5 |
BN (mp-984) | <1 1 1> | <1 0 0> | 245.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 61.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 260.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 184.1 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 247.4 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 173.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 55.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 247.4 |
Al (mp-134) | <1 1 0> | <1 0 0> | 184.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 245.5 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 1> | 164.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 220.3 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 205.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 275.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 275.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 165.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 330.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 275.4 |
Al (mp-134) | <1 0 0> | <1 1 0> | 260.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 110.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 220.3 |
C (mp-66) | <1 1 1> | <1 0 1> | 247.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 275.4 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 86.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 184.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 245.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NbSb3O8 (mp-760134) | 0.6145 | 0.005 | 3 |
TaSb3O8 (mp-759172) | 0.6109 | 0.003 | 3 |
Sb2WO6 (mp-541435) | 0.5396 | 0.000 | 3 |
Ag3RuO4 (mp-510453) | 0.3196 | 0.066 | 3 |
Ba3(YI6)2 (mp-776579) | 0.6081 | 0.078 | 3 |
Ca3Fe2(WO6)2 (mvc-13104) | 0.6493 | 0.038 | 4 |
Mg2SnWO6 (mvc-5015) | 0.7234 | 0.156 | 4 |
Li2Nb6NiO18 (mp-769462) | 0.7464 | 0.073 | 4 |
AlNi(WO4)2 (mvc-613) | 0.6614 | 0.231 | 4 |
LiNi(WO4)2 (mp-25603) | 0.7272 | 0.090 | 4 |
SbO2 (mp-230) | 0.7104 | 0.000 | 2 |
NaLaMgTeO6 (mp-9239) | 0.7452 | 0.000 | 5 |
Sr5La2Mn8(O3F)6 (mp-743681) | 0.7030 | 0.592 | 5 |
Hg12SbBr(ClO3)2 (mp-642625) | 0.7461 | 0.032 | 5 |
Li3La8Ti9Cr3O36 (mp-743640) | 0.6765 | 0.066 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Ir O |
Final Energy/Atom-4.9320 eV |
Corrected Energy-169.0608 eV
-169.0608 eV = -157.8242 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)