Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.815 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZrO2 |
Band Gap3.463 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 227.3 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 312.6 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 255.7 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 28.4 |
C (mp-48) | <1 1 0> | <1 0 0> | 166.7 |
KP(HO2)2 (mp-23959) | <1 1 1> | <1 1 0> | 155.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 255.7 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 113.7 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 142.1 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 113.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 184.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 255.7 |
WSe2 (mp-1821) | <0 0 1> | <0 1 1> | 308.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 1> | 308.2 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 109.4 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 1> | 308.2 |
Cu (mp-30) | <1 1 1> | <0 1 0> | 273.4 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 312.6 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 1> | 184.9 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 1> | 248.9 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 85.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 85.2 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 184.9 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 28.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 142.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 184.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 227.3 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 0 1> | 187.2 |
YAlO3 (mp-3792) | <0 1 0> | <1 1 0> | 78.0 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 164.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 312.6 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 312.6 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 164.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 142.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 277.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 113.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 227.3 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 1> | 308.2 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 109.4 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 198.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 62.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 277.8 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 255.7 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 218.8 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 222.2 |
ZnO (mp-2133) | <1 1 1> | <1 1 1> | 248.9 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 85.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 222.2 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 109.4 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 312.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
279 | 100 | 161 | 0 | 0 | 0 |
100 | 339 | 146 | 0 | 0 | 0 |
161 | 146 | 350 | 0 | 0 | 0 |
0 | 0 | 0 | 115 | 0 | 0 |
0 | 0 | 0 | 0 | 86 | 0 |
0 | 0 | 0 | 0 | 0 | 63 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
5.0 | -0.6 | -2.1 | 0 | 0 | 0 |
-0.6 | 3.7 | -1.3 | 0 | 0 | 0 |
-2.1 | -1.3 | 4.3 | 0 | 0 | 0 |
0 | 0 | 0 | 8.7 | 0 | 0 |
0 | 0 | 0 | 0 | 11.6 | 0 |
0 | 0 | 0 | 0 | 0 | 15.8 |
Shear Modulus GV90 GPa |
Bulk Modulus KV198 GPa |
Shear Modulus GR85 GPa |
Bulk Modulus KR193 GPa |
Shear Modulus GVRH88 GPa |
Bulk Modulus KVRH195 GPa |
Elastic Anisotropy0.32 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TaNO (mp-4165) | 0.2805 | 0.000 | 3 |
CeZr11O24 (mp-752706) | 0.2795 | 0.017 | 3 |
VOF (mp-768037) | 0.2835 | 0.012 | 3 |
ScOF (mp-4661) | 0.2921 | 0.000 | 3 |
NbNO (mp-7596) | 0.3002 | 0.000 | 3 |
ZrO2 (mp-2858) | 0.1913 | 0.000 | 2 |
HfO2 (mp-775757) | 0.0641 | 0.010 | 2 |
HfO2 (mp-352) | 0.2147 | 0.000 | 2 |
NdO2 (mp-755820) | 0.3242 | 0.169 | 2 |
CeSe2 (mp-1080303) | 0.3388 | 0.024 | 2 |
Explore more synthesis descriptions for materials of composition ZrO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv O |
Final Energy/Atom-9.4947 eV |
Corrected Energy-239.1085 eV
-239.1085 eV = -227.8719 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)