Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.339 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.717 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 210.0 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 124.0 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 226.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 124.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 226.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 226.5 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 169.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 124.0 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 185.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 302.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 226.5 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 124.0 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 154.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 154.9 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 258.7 |
C (mp-66) | <1 1 0> | <0 1 0> | 302.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 129.3 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 248.0 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 169.7 |
GaP (mp-2490) | <1 1 0> | <0 1 0> | 302.0 |
GaP (mp-2490) | <1 1 1> | <1 0 0> | 105.0 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 226.5 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 302.0 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 0> | 302.0 |
Cu (mp-30) | <1 0 0> | <1 0 1> | 169.7 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 248.0 |
LiAlO2 (mp-3427) | <1 0 1> | <1 0 0> | 210.0 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 124.0 |
CaF2 (mp-2741) | <1 1 0> | <0 1 0> | 302.0 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 124.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 302.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 0> | 302.0 |
Si (mp-149) | <1 1 0> | <0 0 1> | 124.0 |
C (mp-48) | <0 0 1> | <0 1 0> | 302.0 |
C (mp-48) | <1 0 0> | <1 0 0> | 210.0 |
WSe2 (mp-1821) | <1 0 1> | <0 0 1> | 248.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 226.5 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 226.5 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 210.0 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 226.5 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 248.0 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 248.0 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 0> | 258.7 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 302.0 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 124.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu(PO3)3 (mp-779530) | 0.5132 | 0.039 | 3 |
Ni(PO3)3 (mp-767052) | 0.5615 | 0.051 | 3 |
Sn2(PO3)5 (mp-26950) | 0.4668 | 0.040 | 3 |
Fe(PO3)3 (mp-540314) | 0.5622 | 0.045 | 3 |
Mn(PO3)3 (mp-704236) | 0.4966 | 0.103 | 3 |
K2Cu(PO3)4 (mp-6598) | 0.4189 | 0.000 | 4 |
LiNi(PO3)5 (mp-705004) | 0.4531 | 0.100 | 4 |
LiCu(PO3)4 (mp-26262) | 0.3752 | 0.000 | 4 |
Na2Cu(PO3)4 (mp-557171) | 0.4057 | 0.000 | 4 |
LiCu(PO3)4 (mp-757306) | 0.4112 | 0.013 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.6426 | 0.087 | 5 |
RbLiV(PO4)2 (mp-764302) | 0.7467 | 0.057 | 5 |
KEu2Si4O10F (mp-561529) | 0.6998 | 0.000 | 5 |
LiAg2P3(HO5)2 (mp-695951) | 0.6453 | 0.020 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Cu_pv P O |
Final Energy/Atom-6.6730 eV |
Corrected Energy-256.7176 eV
Uncorrected energy = -240.2296 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Corrected energy = -256.7176 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)