Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.085 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.152 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVF4 |
Band Gap2.410 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 104.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 301.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 139.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 174.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 60.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 148.0 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 67.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 313.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 174.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 174.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 58.1 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 181.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 67.7 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 301.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 139.2 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 60.4 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 58.1 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 290.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 243.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 174.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 104.4 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 228.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 304.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 348.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 135.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 208.8 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 148.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 345.3 |
BN (mp-984) | <1 0 1> | <1 0 1> | 203.1 |
BN (mp-984) | <1 1 0> | <0 1 1> | 301.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 290.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 232.3 |
Al (mp-134) | <1 1 0> | <0 1 1> | 181.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 34.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 1> | 167.5 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 313.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 290.4 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 0> | 246.6 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 270.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 232.3 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 58.1 |
C (mp-66) | <1 0 0> | <1 0 1> | 270.8 |
C (mp-66) | <1 1 0> | <1 1 1> | 251.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 246.6 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 67.7 |
Mg (mp-153) | <1 0 1> | <0 1 1> | 301.8 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 1> | 135.4 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 1> | 135.4 |
LaF3 (mp-905) | <1 0 0> | <1 1 1> | 167.5 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 152.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgVF4 (mvc-3716) | 0.5407 | 0.097 | 3 |
MgTe2O5 (mp-5746) | 0.6311 | 0.007 | 3 |
LiMnF4 (mp-764361) | 0.5908 | 0.026 | 3 |
Li2AgF5 (mp-758134) | 0.5927 | 0.056 | 3 |
ZnWO4 (mp-561591) | 0.5051 | 0.041 | 3 |
LiVOF3 (mp-764199) | 0.5915 | 0.078 | 4 |
YCu(WO4)2 (mvc-16327) | 0.6682 | 0.033 | 4 |
YV(WO4)2 (mvc-594) | 0.6607 | 0.190 | 4 |
YSn(WO4)2 (mvc-601) | 0.6214 | 0.074 | 4 |
YTa(WO4)2 (mvc-612) | 0.6426 | 0.297 | 4 |
SbO2 (mvc-6570) | 0.7369 | 0.137 | 2 |
Li4NbTe2WO12 (mp-763988) | 0.7035 | 0.075 | 5 |
LaTaZnCrO6 (mvc-9887) | 0.7119 | 0.267 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv F |
Final Energy/Atom-5.5836 eV |
Corrected Energy-148.1973 eV
Uncorrected energy = -134.0053 eV
Composition-based energy adjustment (-0.462 eV/atom x 16.0 atoms) = -7.3920 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -148.1973 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)