Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.021 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.420 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeO2 + LiF |
Band Gap2.004 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 299.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 204.5 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 272.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 139.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 -1> | 211.5 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 279.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 232.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 232.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 139.4 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 349.3 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 136.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 139.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 349.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 199.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 185.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 139.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 325.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 179.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 139.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 215.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 268.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 349.3 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 349.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 232.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 278.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 325.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 199.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 249.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 249.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 349.3 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 204.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 325.2 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 149.7 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 349.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 199.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 325.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 179.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 278.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 278.7 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 249.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 92.9 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 272.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 139.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 232.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 249.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 249.5 |
BN (mp-984) | <1 1 1> | <0 1 0> | 99.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 46.5 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 149.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 249.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiCoO2 (mp-868388) | 0.2086 | 0.085 | 3 |
LiVO2 (mp-764772) | 0.2015 | 0.048 | 3 |
Li3SbS4 (mp-752426) | 0.1904 | 0.062 | 3 |
LiCr2O3 (mp-769787) | 0.2268 | 0.078 | 3 |
LiFeO2 (mp-771995) | 0.2120 | 0.027 | 3 |
Li24Mn11CrO36 (mp-770622) | 0.2223 | 0.001 | 4 |
Li5Cr2Co3O10 (mp-775237) | 0.2151 | 0.092 | 4 |
Li24Mn11CrO36 (mp-770619) | 0.2176 | 0.001 | 4 |
Li5Fe3(CoO5)2 (mp-761617) | 0.2158 | 0.081 | 4 |
Li3FeOF3 (mp-777934) | 0.2202 | 0.416 | 4 |
Te2Au (mp-1662) | 0.4704 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3687 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.4051 | 0.009 | 2 |
Sb2Te3 (mp-1080789) | 0.5053 | 0.129 | 2 |
Te2Au (mp-567525) | 0.4721 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4307 | 0.005 | 5 |
Na (mp-999501) | 0.7008 | 0.116 | 1 |
Sb (mp-632286) | 0.5794 | 0.059 | 1 |
Bi (mp-567379) | 0.6638 | 0.062 | 1 |
Te (mp-570459) | 0.5577 | 0.044 | 1 |
Te (mp-105) | 0.6424 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.2658 eV |
Corrected Energy-142.9284 eV
-142.9284 eV = -126.3780 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)