Final Magnetic Moment5.784 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.790 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi5(PO5)4 + VPO4 + TiP2O7 + Sb |
Band Gap0.029 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 197.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 267.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 200.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 200.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 200.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 267.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 200.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 67.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 200.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 200.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 200.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 200.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 200.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 267.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 267.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 267.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 67.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 200.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 267.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 67.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 200.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 186.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 200.9 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 200.9 |
Si (mp-149) | <1 1 1> | <0 0 1> | 200.9 |
Au (mp-81) | <1 1 1> | <0 0 1> | 267.9 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 267.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 67.0 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 267.9 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 67.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 67.0 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 267.9 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 1> | 197.7 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 267.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 67.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 267.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 267.9 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 267.9 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 67.0 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 67.0 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 200.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 267.9 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 67.0 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 267.9 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 267.9 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 67.0 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 67.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.3195 | 0.050 | 3 |
VPO4 (mp-861584) | 0.2411 | 0.076 | 3 |
MnPO4 (mp-504382) | 0.3941 | 0.070 | 3 |
FePO4 (mp-773675) | 0.3553 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.2685 | 0.077 | 3 |
TiNi(PO4)2 (mp-761309) | 0.1648 | 0.018 | 4 |
MnV(PO4)2 (mp-770182) | 0.1609 | 0.003 | 4 |
TiV(PO4)2 (mp-850923) | 0.1667 | 0.000 | 4 |
TiMn(PO4)2 (mp-773171) | 0.1349 | 0.015 | 4 |
V5Co(PO4)6 (mp-790064) | 0.1657 | 0.106 | 4 |
Cr5O12 (mp-19575) | 0.7462 | 0.025 | 2 |
MoO2 (mvc-6944) | 0.7495 | 0.281 | 2 |
Ti3V2Cu(PO4)6 (mp-766633) | 0.1166 | 0.068 | 5 |
Ti3Mn2Sb(PO4)6 (mp-776000) | 0.0937 | 0.051 | 5 |
Ti3Fe2Sb(PO4)6 (mp-778503) | 0.0405 | 0.058 | 5 |
Ti3MnCo2(PO4)6 (mp-778393) | 0.1093 | 0.062 | 5 |
Ti3MnV2(PO4)6 (mp-774314) | 0.0883 | 0.016 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5149 | 0.065 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.5304 | 0.009 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5289 | 0.011 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.3532 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4745 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Ti_pv V_pv Sb P O |
Final Energy/Atom-7.7067 eV |
Corrected Energy-297.6616 eV
-297.6616 eV = -277.4426 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 3.3640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)