Final Magnetic Moment7.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.549 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrPO4 + VPO4 + Sn3(PO4)2 + SnP2O7 + SnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LiF (mp-1138) | <1 1 1> | <0 0 1> | 256.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 320.5 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 192.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 320.5 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 193.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 320.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 192.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 192.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 64.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 192.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 192.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 128.2 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 192.3 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 320.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 256.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 320.5 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 320.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 320.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 256.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 192.3 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 256.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 256.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 256.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 64.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 192.3 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 64.1 |
C (mp-48) | <0 0 1> | <0 0 1> | 256.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 256.4 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 256.4 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 256.4 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 192.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 256.4 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 192.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 64.1 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 192.3 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 256.4 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 320.5 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 320.5 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 192.3 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 320.5 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 192.3 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 64.1 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 256.4 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 64.1 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 320.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2Cr3O12 (mp-764449) | 0.4996 | 0.216 | 3 |
MnPO4 (mp-773411) | 0.4337 | 0.344 | 3 |
Cr3(CoO6)2 (mp-861261) | 0.5152 | 0.096 | 3 |
Fe2(PO4)3 (mp-31866) | 0.5053 | 0.451 | 3 |
Mo2(PO4)3 (mp-704253) | 0.4959 | 0.001 | 3 |
NaTi2(PO4)3 (mp-6761) | 0.1996 | 0.000 | 4 |
Ti2Sn(PO4)3 (mp-773911) | 0.1292 | 0.006 | 4 |
V2Sn(PO4)3 (mp-853198) | 0.0818 | 0.094 | 4 |
NaSn2(PO4)3 (mp-22163) | 0.1923 | 0.001 | 4 |
CaTi4(PO4)6 (mp-16831) | 0.1793 | 0.000 | 4 |
Cr5O12 (mp-773920) | 0.6457 | 0.000 | 2 |
Mo4O11 (mp-565865) | 0.7432 | 0.026 | 2 |
V5O12 (mp-778252) | 0.6181 | 0.024 | 2 |
V3FeSn2(PO4)6 (mp-851232) | 0.0703 | 0.058 | 5 |
V3CoSn2(PO4)6 (mp-775609) | 0.1105 | 0.084 | 5 |
SrTiFe(PO4)3 (mp-743630) | 0.1228 | 0.146 | 5 |
Na2Ti3Cr(PO4)6 (mp-773611) | 0.1769 | 0.016 | 5 |
Ti3CrSn2(PO4)6 (mp-777023) | 0.0739 | 0.002 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5408 | 0.068 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.3545 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.4137 | 0.001 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.4578 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.4628 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: V_pv Cr_pv Sn_d P O |
Final Energy/Atom-7.3335 eV |
Corrected Energy-287.9193 eV
-287.9193 eV = -264.0054 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 7.0590 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)