Final Magnetic Moment0.953 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.588 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.185 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2MnVP2(O4F)2 |
Band Gap0.319 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 177.7 |
Te2W (mp-22693) | <1 1 1> | <1 0 1> | 224.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 323.1 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 224.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 224.2 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 296.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 300.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 138.5 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 230.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 276.7 |
BN (mp-984) | <1 0 0> | <0 0 1> | 323.1 |
BN (mp-984) | <1 0 1> | <1 1 1> | 222.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 323.1 |
BN (mp-984) | <1 1 1> | <1 1 0> | 240.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 276.9 |
Al (mp-134) | <1 1 1> | <1 1 1> | 222.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 138.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 332.0 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 1> | 224.2 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 236.9 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 221.3 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 236.9 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 141.6 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 332.0 |
SiC (mp-7631) | <1 0 1> | <1 1 0> | 240.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 184.6 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 180.3 |
TiO2 (mp-2657) | <1 0 1> | <1 1 0> | 180.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 230.8 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 230.8 |
C (mp-66) | <1 0 0> | <1 -1 0> | 292.8 |
C (mp-66) | <1 1 0> | <1 1 0> | 180.3 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 296.1 |
Mg (mp-153) | <1 0 0> | <1 -1 1> | 217.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 230.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 230.8 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 323.1 |
LaF3 (mp-905) | <1 0 1> | <1 -1 1> | 217.2 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 296.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 236.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 323.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 138.5 |
AlN (mp-661) | <1 1 1> | <1 -1 0> | 195.2 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 276.9 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 276.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 323.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 276.9 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 224.2 |
GaN (mp-804) | <1 0 0> | <1 -1 1> | 217.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 230.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr5(PO4)4 (mp-540446) | 0.5616 | 0.007 | 3 |
Mg2V2O7 (mp-32500) | 0.5939 | 0.000 | 3 |
Cr5(PO4)4 (mp-775246) | 0.5615 | 0.007 | 3 |
V7(PO4)6 (mp-769607) | 0.6224 | 0.020 | 3 |
Cr7(PO4)6 (mp-505154) | 0.5878 | 0.002 | 3 |
LiPWO5 (mp-763520) | 0.3790 | 0.035 | 4 |
Li3Ni2(PO4)3 (mp-504271) | 0.4464 | 0.065 | 4 |
LiNbPO5 (mp-757734) | 0.4316 | 0.084 | 4 |
LiMoPO5 (mp-540137) | 0.2785 | 0.002 | 4 |
Li3Mn4(PO4)6 (mp-767970) | 0.4861 | 0.150 | 4 |
LiCoPO4F (mp-25487) | 0.2355 | 0.095 | 5 |
LiCrPO4F (mp-25501) | 0.2394 | 0.000 | 5 |
LiFePO4F (mp-25515) | 0.2145 | 0.000 | 5 |
LiMnPO4F (mp-25552) | 0.2256 | 0.000 | 5 |
LiVPO4F (mp-25619) | 0.2080 | 0.000 | 5 |
Li2MnVP2(O4F)2 (mp-777226) | 0.1638 | 0.029 | 6 |
Li2MnVP2(O4F)2 (mp-777436) | 0.1727 | 0.150 | 6 |
Li2MnVP2(O4F)2 (mp-777197) | 0.1471 | 0.200 | 6 |
Li2MnVP2(O4F)2 (mp-792971) | 0.1674 | 0.163 | 6 |
Li2MnVP2(O4F)2 (mp-776709) | 0.1522 | 0.024 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O F |
Final Energy/Atom-6.7335 eV |
Corrected Energy-233.4332 eV
-233.4332 eV = -215.4709 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 6.7257 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)