Final Magnetic Moment0.030 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.163 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.232 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeS + FeS2 + Li2S |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 72.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 288.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 288.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 72.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 288.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 216.4 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 124.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 216.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 288.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 248.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 288.6 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 288.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 216.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 144.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 216.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 216.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 143.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 216.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 288.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 72.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 216.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 288.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 216.4 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 288.6 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 216.4 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 288.6 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 216.4 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 216.4 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 216.4 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 288.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 288.6 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 216.4 |
Ga2O3 (mp-886) | <1 1 -1> | <0 1 0> | 248.6 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 288.6 |
C (mp-48) | <1 0 0> | <0 1 0> | 248.6 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 216.4 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 216.4 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 288.6 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 288.6 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 288.6 |
CsI (mp-614603) | <1 1 1> | <0 0 1> | 216.4 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 216.4 |
LiAlO2 (mp-3427) | <1 1 0> | <0 1 1> | 143.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na5CuO4 (mp-779650) | 0.5299 | 0.080 | 3 |
Li2Cu2S3 (mp-774762) | 0.4522 | 0.081 | 3 |
Li3(FeS2)2 (mp-753818) | 0.5246 | 0.170 | 3 |
Na5FeS4 (mp-556086) | 0.4449 | 0.136 | 3 |
Na2Mn2Se3 (mp-29745) | 0.5365 | 0.000 | 3 |
Li7VO5F (mp-764214) | 0.5532 | 0.081 | 4 |
Li7MnO5F (mp-766915) | 0.4720 | 0.096 | 4 |
Na2Li2CoO4 (mp-763254) | 0.5834 | 0.073 | 4 |
Sr2Li2NiO4 (mp-769674) | 0.5048 | 0.091 | 4 |
Na2Li2FeO4 (mp-25538) | 0.5597 | 0.060 | 4 |
CoSb2 (mp-755) | 0.6236 | 0.002 | 2 |
Bi2Rh (mp-23217) | 0.6385 | 0.000 | 2 |
Re2P5 (mp-27736) | 0.6481 | 0.000 | 2 |
CoAs2 (mp-2715) | 0.6359 | 0.000 | 2 |
P3Ru (mp-28400) | 0.5406 | 0.000 | 2 |
Li4NbTe2WO12 (mp-763988) | 0.7440 | 0.075 | 5 |
NaZr2SN2Cl (mp-679669) | 0.6447 | 0.077 | 5 |
Li4Nb2Fe3Te3O16 (mp-765556) | 0.7083 | 0.092 | 5 |
LaMgFeAgO6 (mvc-8987) | 0.7303 | 0.091 | 5 |
Sr2AlCu2BiO7 (mvc-306) | 0.7363 | 0.103 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Fe_pv S |
Final Energy/Atom-4.3539 eV |
Corrected Energy-369.5395 eV
-369.5395 eV = -348.3088 eV (uncorrected energy) - 21.2307 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)