Final Magnetic Moment18.961 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.220 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi24Mn11CrO36 + LiCrSnO4 + LiMnCrO4 + MnCr2O4 + SnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 232.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.0 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 115.4 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 117.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 99.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 262.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 245.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 291.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 245.9 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 115.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 199.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 307.4 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 199.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 184.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 307.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 174.6 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 184.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 174.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 291.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 298.9 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 255.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 123.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 307.4 |
BN (mp-984) | <1 0 1> | <1 1 1> | 262.1 |
BN (mp-984) | <1 1 0> | <0 1 1> | 234.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 184.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 298.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 245.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 307.4 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 232.8 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 230.8 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 234.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 184.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 255.5 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 234.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 307.4 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 298.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 184.4 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 174.6 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.5 |
C (mp-66) | <1 0 0> | <1 0 1> | 255.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 0> | 115.4 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 170.3 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 262.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 184.4 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 298.9 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 99.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn2O4 (mp-771583) | 0.1908 | 0.049 | 3 |
Li(FeO2)2 (mp-771571) | 0.1259 | 0.666 | 3 |
LiCr2O4 (mp-771523) | 0.2047 | 0.088 | 3 |
Li(NiO2)2 (mp-771429) | 0.1766 | 0.063 | 3 |
LiTi2O4 (mp-776170) | 0.1793 | 0.042 | 3 |
Li4Mn3Cr5O16 (mp-771517) | 0.1323 | 0.039 | 4 |
Li4V3Fe5O16 (mp-772417) | 0.1271 | 0.077 | 4 |
Li4Mn5Cr3O16 (mp-772402) | 0.1227 | 0.054 | 4 |
Li4Mn3Fe5O16 (mp-772388) | 0.1188 | 0.048 | 4 |
Li4Cr3Fe5O16 (mp-772464) | 0.1357 | 0.899 | 4 |
Si3N4 (mp-641539) | 0.2990 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.3100 | 0.208 | 2 |
Fe3O4 (mp-542433) | 0.3407 | 0.075 | 2 |
Cr3N4 (mp-1014358) | 0.2911 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.3240 | 0.060 | 2 |
Li4Mn3Fe2Co3O16 (mp-775386) | 0.1112 | 0.068 | 5 |
Li4Mn3Cr3(FeO8)2 (mp-761449) | 0.1079 | 0.570 | 5 |
Li4V3Cr3(SnO8)2 (mp-777670) | 0.0993 | 0.000 | 5 |
Li4Fe3Co3(SnO8)2 (mp-793779) | 0.1033 | 0.072 | 5 |
Li4Cr3Co3(SnO8)2 (mp-778219) | 0.1059 | 0.035 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7049 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7076 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7156 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7100 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7131 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Cr_pv Sn_d O |
Final Energy/Atom-6.8255 eV |
Corrected Energy-213.4335 eV
-213.4335 eV = -191.1154 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 11.0816 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)