Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.124 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb2O |
Band Gap0.938 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 291.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 243.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 286.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 340.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 340.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 291.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 291.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 145.9 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 209.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 141.9 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 286.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 266.6 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 185.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 286.6 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 104.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 340.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 340.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 266.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 209.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 141.9 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 107.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 340.4 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 278.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 291.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 340.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 107.2 |
Al (mp-134) | <1 1 1> | <1 1 1> | 141.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 291.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 291.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 209.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 243.2 |
Al (mp-134) | <1 1 0> | <0 1 1> | 209.8 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 194.5 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 278.9 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 340.4 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 340.4 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 209.8 |
C (mp-66) | <1 1 0> | <1 0 1> | 107.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 266.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 340.4 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 1> | 107.2 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 185.9 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 266.6 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 340.4 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 194.5 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 340.4 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 145.9 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 243.2 |
NdGaO3 (mp-3196) | <0 1 1> | <1 1 0> | 266.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BiOF (mp-753478) | 0.4472 | 0.019 | 3 |
CeZr7O16 (mp-752503) | 0.4902 | 0.024 | 3 |
CeZr11O24 (mp-752706) | 0.4577 | 0.017 | 3 |
DySCl (mp-561307) | 0.5190 | 0.000 | 3 |
Zr15VO32 (mp-765884) | 0.4911 | 0.015 | 3 |
HfO2 (mp-685097) | 0.3268 | 0.029 | 2 |
YbCl2 (mp-23220) | 0.2428 | 0.010 | 2 |
SnO2 (mp-560417) | 0.2577 | 0.134 | 2 |
K2O (mp-776016) | 0.1711 | 0.020 | 2 |
HfO2 (mp-1858) | 0.1858 | 0.024 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv O |
Final Energy/Atom-3.1931 eV |
Corrected Energy-82.2526 eV
-82.2526 eV = -76.6343 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)