Final Magnetic Moment13.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.824 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.020 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi4Mn(PO4)6 + Fe3(PO4)2 + Mn3(PO4)2 |
Band Gap1.127 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 263.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 329.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 197.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 197.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.9 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 193.1 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 263.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 197.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 197.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 197.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 263.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 263.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 263.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 263.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 197.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 197.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 197.8 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 263.7 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 263.7 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 1> | 193.1 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 65.9 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 263.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 181.5 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 329.6 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 329.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 197.8 |
SiC (mp-8062) | <1 0 0> | <1 0 1> | 193.1 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 329.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 197.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.9 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 65.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 329.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 329.6 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 263.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.9 |
GaSb (mp-1156) | <1 0 0> | <1 0 1> | 193.1 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 263.7 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 65.9 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 65.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 329.6 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 263.7 |
Ni (mp-23) | <1 1 1> | <1 0 1> | 193.1 |
PbSe (mp-2201) | <1 0 0> | <1 0 1> | 193.1 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.9 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 329.6 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 263.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.2679 | 0.344 | 3 |
VPO4 (mp-861584) | 0.1879 | 0.079 | 3 |
FePO4 (mp-773675) | 0.3470 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.2201 | 0.077 | 3 |
CrCdO4 (mp-19630) | 0.4085 | 0.013 | 3 |
TiFe(PO4)2 (mp-761424) | 0.0924 | 0.144 | 4 |
TiNi(PO4)2 (mp-761309) | 0.1100 | 0.012 | 4 |
TiV(PO4)2 (mp-850923) | 0.0990 | 0.002 | 4 |
TiMn(PO4)2 (mp-773171) | 0.1274 | 0.015 | 4 |
V5Co(PO4)6 (mp-790064) | 0.1355 | 0.060 | 4 |
Mo4O11 (mp-565865) | 0.7412 | 0.026 | 2 |
MoO2 (mvc-6944) | 0.7278 | 0.281 | 2 |
Ti3V2Co(PO4)6 (mp-775650) | 0.0716 | 0.040 | 5 |
Ti3Fe2Cu(PO4)6 (mp-777685) | 0.0696 | 0.055 | 5 |
Ti3MnCo2(PO4)6 (mp-778393) | 0.0605 | 0.036 | 5 |
Ti3FeNi2(PO4)6 (mp-778326) | 0.0712 | 0.019 | 5 |
Ti3MnV2(PO4)6 (mp-774314) | 0.0529 | 0.016 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.5126 | 0.068 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.5413 | 0.009 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5396 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.2988 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4667 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Ti_pv Mn_pv Fe_pv P O |
Final Energy/Atom-7.7409 eV |
Corrected Energy-302.6750 eV
-302.6750 eV = -278.6732 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 7.1469 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)