Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.803 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.070 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeF2 + LiF |
Band Gap3.092 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 138.6 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 234.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 168.0 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 138.6 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 207.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 277.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 138.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 234.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 264.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 138.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 162.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 234.0 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 216.0 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 335.9 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 264.4 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 234.0 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 234.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 270.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 207.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 268.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 264.4 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 312.0 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 69.3 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 312.0 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 234.0 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 78.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 277.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 88.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 264.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 279.9 |
GaSe (mp-1943) | <1 1 0> | <0 1 1> | 234.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 324.0 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 268.0 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 264.4 |
BN (mp-984) | <1 0 0> | <1 1 1> | 209.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 270.0 |
BN (mp-984) | <1 1 0> | <1 1 0> | 268.0 |
BN (mp-984) | <1 1 1> | <1 1 0> | 268.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 270.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 176.3 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 270.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 216.0 |
Te2Mo (mp-602) | <1 1 1> | <0 1 0> | 279.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 324.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 168.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 88.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 335.9 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 277.1 |
GaSe (mp-1943) | <1 1 1> | <0 1 1> | 234.0 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 216.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn2F5 (mp-777631) | 0.3597 | 0.069 | 3 |
Al10Ge2O19 (mp-28499) | 0.6542 | 0.031 | 3 |
Mn2V2O7 (mp-572632) | 0.6851 | 0.004 | 3 |
Fe4Bi2O9 (mp-540741) | 0.6782 | 0.012 | 3 |
Al2SiO5 (mp-4934) | 0.6315 | 0.007 | 3 |
LiFe2O2F3 (mp-780549) | 0.5932 | 0.070 | 4 |
Li3Cr2(PO4)3 (mp-775597) | 0.6637 | 0.005 | 4 |
Li2V(PO4)2 (mp-540312) | 0.6502 | 0.056 | 4 |
LiCrPO5 (mp-850227) | 0.5648 | 0.065 | 4 |
LiMnPO5 (mp-761641) | 0.6176 | 0.071 | 4 |
Li2VP2HO8 (mp-780754) | 0.6470 | 0.001 | 5 |
Li2FeP2HO8 (mp-767473) | 0.6517 | 0.000 | 5 |
NaMg3Al(MoO4)5 (mp-561496) | 0.6878 | 0.007 | 5 |
Li2MnP2HO8 (mp-781059) | 0.6434 | 0.005 | 5 |
Li3V2P4(HO8)2 (mp-776714) | 0.6772 | 0.000 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.7238 | 0.054 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv F |
Final Energy/Atom-5.3638 eV |
Corrected Energy-193.5062 eV
-193.5062 eV = -171.6422 eV (uncorrected energy) - 21.8640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)