Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.388 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoPO4 |
Band Gap2.836 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 174.4 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 160.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 31.7 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 54.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 285.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 239.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 174.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 158.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 285.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 66.2 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 239.9 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 239.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 54.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 274.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 316.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 58.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 221.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 174.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 316.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 221.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 221.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 348.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 331.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 126.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 58.1 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 290.7 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 269.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 253.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 269.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 232.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 293.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 253.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 264.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 66.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 198.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 316.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 221.6 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 264.8 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 160.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 66.2 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 290.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 253.3 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 198.6 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 219.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 95.0 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 219.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 126.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 58.1 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 293.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 158.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3BO6 (mp-770370) | 0.4678 | 0.007 | 3 |
Cr(AgO2)2 (mp-557056) | 0.4525 | 0.016 | 3 |
Li2SO4 (mp-558382) | 0.3760 | 0.055 | 3 |
Na2CrO4 (mp-18779) | 0.4650 | 0.000 | 3 |
Mn(AgO2)2 (mp-554049) | 0.4096 | 0.185 | 3 |
LiMnPO4 (mp-777038) | 0.1741 | 0.039 | 4 |
LiNiPO4 (mp-762168) | 0.1427 | 0.022 | 4 |
LiCrPO4 (mp-761392) | 0.2377 | 0.023 | 4 |
LiVPO4 (mp-761298) | 0.2421 | 0.030 | 4 |
LiCrPO4 (mp-31664) | 0.3295 | 0.023 | 4 |
Li7Mn7P6(O8F)3 (mp-763896) | 0.4016 | 0.032 | 5 |
Li7V7P6(O8F)3 (mp-763895) | 0.4299 | 0.023 | 5 |
Li7Fe7P6(O8F)3 (mp-997551) | 0.4109 | 0.023 | 5 |
Li4V2Si(PO6)2 (mp-770404) | 0.5245 | 0.085 | 5 |
Li7Cr7P6(O8F)3 (mp-763893) | 0.4979 | 0.026 | 5 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.6664 | 0.010 | 6 |
Explore more synthesis descriptions for materials of composition LiCoPO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O |
Final Energy/Atom-6.6000 eV |
Corrected Energy-203.5314 eV
-203.5314 eV = -184.7988 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)