Final Magnetic Moment13.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.526 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.062 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2FeCo3O8 + LiO8 + LiCuO2 + Li(CoO2)2 + Fe2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 288.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 110.4 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 161.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 116.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 220.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 112.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 331.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 165.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 58.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 116.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 58.2 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 192.2 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 192.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 174.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 174.5 |
Al (mp-134) | <1 0 0> | <1 0 0> | 165.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 58.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 112.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 250.7 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 192.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 161.1 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 232.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 165.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 232.6 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 1> | 224.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 174.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 288.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 161.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 55.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 165.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 165.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 276.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 165.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 58.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 174.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 116.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 174.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 276.0 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 276.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 55.2 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 331.2 |
C (mp-66) | <1 1 0> | <0 1 0> | 288.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 174.5 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 161.1 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 1> | 112.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 55.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.1909 | 0.666 | 3 |
Ca(MoO2)2 (mvc-6227) | 0.2029 | 0.228 | 3 |
Ca(AgO2)2 (mvc-4859) | 0.2177 | 0.228 | 3 |
Li9Mn15O32 (mp-769450) | 0.1869 | 0.866 | 3 |
LiFe5O8 (mp-706252) | 0.2044 | 0.645 | 3 |
Li4Ti3Fe5O16 (mp-771498) | 0.1533 | 0.433 | 4 |
Li4Mn3Fe5O16 (mp-772388) | 0.1514 | 0.048 | 4 |
Li4Fe5Co3O16 (mp-773387) | 0.1215 | 0.072 | 4 |
Li4Fe5Sn3O16 (mp-769745) | 0.1461 | 0.074 | 4 |
Li4Mn5Co3O16 (mp-771231) | 0.1588 | 0.127 | 4 |
Fe3O4 (mp-542433) | 0.3433 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.3141 | 0.060 | 2 |
Fe3O4 (mp-715558) | 0.3488 | 0.785 | 2 |
Fe3O4 (mp-716052) | 0.3541 | 0.781 | 2 |
Fe3O4 (mp-715811) | 0.3520 | 0.037 | 2 |
Li4Fe2Co3Ni3O16 (mp-775701) | 0.1203 | 0.039 | 5 |
Li4Fe3Co3(NiO8)2 (mp-764308) | 0.1084 | 0.054 | 5 |
Li4Mn3Fe3(CuO8)2 (mp-767314) | 0.1242 | 0.056 | 5 |
Li4Mn3Fe2Cu3O16 (mp-779210) | 0.1203 | 0.034 | 5 |
Li4Ti3Co3(NiO8)2 (mp-763517) | 0.1194 | 0.054 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7284 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7140 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7212 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7249 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7261 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Co Cu_pv O |
Final Energy/Atom-5.6931 eV |
Corrected Energy-184.4654 eV
-184.4654 eV = -159.4078 eV (uncorrected energy) - 13.8210 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)