Final Magnetic Moment0.112 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.645 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.533 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVF4 + VF3 + LiV3(OF3)2 |
Band Gap1.028 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 119.4 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 199.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 293.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 143.4 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 50.8 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 28.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 209.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 253.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 159.2 |
KCl (mp-23193) | <1 1 1> | <0 1 -1> | 141.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 258.2 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 159.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 278.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 203.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 229.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 315.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 159.2 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 159.2 |
TePb (mp-19717) | <1 0 0> | <0 1 -1> | 330.6 |
TePb (mp-19717) | <1 1 1> | <0 1 -1> | 141.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 229.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 -1> | 141.7 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 278.6 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 278.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 -1> | 47.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 143.4 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 1> | 152.5 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 125.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 229.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 86.1 |
MoS2 (mp-1434) | <1 0 0> | <0 1 1> | 203.3 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 114.7 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 200.8 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 143.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 290.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 258.2 |
Al (mp-134) | <1 0 0> | <0 1 0> | 278.6 |
Al (mp-134) | <1 1 0> | <0 1 1> | 203.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 86.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 172.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 238.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 344.2 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 203.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 86.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 28.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 101.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 86.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 143.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 229.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 199.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu(TeO3)4 (mp-756573) | 0.4687 | 0.089 | 3 |
V7(WO5)6 (mp-774948) | 0.3929 | 0.098 | 3 |
Ni(TeO3)4 (mp-771470) | 0.4681 | 0.087 | 3 |
Fe(SbO3)4 (mp-770991) | 0.3869 | 0.209 | 3 |
Ti7(WO5)6 (mp-853224) | 0.4467 | 0.068 | 3 |
LiV(TeO4)3 (mp-764954) | 0.3507 | 0.049 | 4 |
LiV4OF11 (mp-780771) | 0.2970 | 0.085 | 4 |
LiV4OF11 (mp-779753) | 0.2524 | 0.457 | 4 |
LiV4OF11 (mp-778629) | 0.2263 | 0.037 | 4 |
LiV4OF11 (mp-779759) | 0.3363 | 0.062 | 4 |
Bi3O7 (mvc-9064) | 0.7338 | 0.141 | 2 |
Sb3O7 (mvc-9074) | 0.7122 | 0.112 | 2 |
LiNbTe2WO12 (mp-764339) | 0.4029 | 0.022 | 5 |
LiNbTe2WO12 (mp-770746) | 0.5373 | 0.025 | 5 |
LiSbTe2WO12 (mp-769943) | 0.5546 | 0.039 | 5 |
LiVTe2WO12 (mp-770705) | 0.3237 | 0.064 | 5 |
LiVTe(WO6)2 (mp-765616) | 0.5708 | 0.048 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.6676 eV |
Corrected Energy-103.7799 eV
-103.7799 eV = -96.3496 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 0.7023 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)