Final Magnetic Moment35.048 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.345 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.107 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeF4 + FeF3 + Fe2O3 |
Band Gap1.441 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2 [3] |
HallP 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 174.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 141.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 70.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 208.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 353.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 306.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 261.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 261.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 353.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 208.9 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 236.0 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 236.0 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 329.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 164.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 208.9 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 229.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 174.5 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 164.7 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 211.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 258.9 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 286.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 174.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 164.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 188.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 70.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 164.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 258.9 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 236.0 |
Al (mp-134) | <1 1 0> | <1 0 1> | 236.0 |
Al (mp-134) | <1 1 1> | <0 1 0> | 353.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 141.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 164.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 174.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 306.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 313.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 353.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 282.4 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 306.0 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 188.3 |
CdTe (mp-406) | <1 1 1> | <0 1 1> | 229.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 261.1 |
TeO2 (mp-2125) | <0 1 0> | <0 1 1> | 286.4 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 156.7 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 286.4 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 156.7 |
TeO2 (mp-2125) | <1 1 1> | <0 1 0> | 211.8 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 211.8 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 188.3 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 232.7 |
SiC (mp-7631) | <1 1 1> | <1 1 0> | 251.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NbFeO4 (mp-608348) | 0.1582 | 0.483 | 3 |
Mn4O7F (mp-780036) | 0.1748 | 0.064 | 3 |
Mn8O13F3 (mp-781602) | 0.1806 | 0.074 | 3 |
Fe2WO6 (mp-25749) | 0.1636 | 0.506 | 3 |
LiCu2F6 (mp-863372) | 0.1215 | 0.034 | 3 |
LiV2OF5 (mp-765048) | 0.1941 | 0.176 | 4 |
LiFe2OF5 (mp-850961) | 0.1715 | 0.552 | 4 |
LiMnFeF6 (mp-566418) | 0.1896 | 0.000 | 4 |
LiFe2OF5 (mp-776722) | 0.1752 | 0.191 | 4 |
LiV2OF5 (mp-861457) | 0.2005 | 0.210 | 4 |
TiO2 (mp-775938) | 0.2118 | 0.039 | 2 |
ZrO2 (mp-775980) | 0.2600 | 0.051 | 2 |
SiO2 (mp-10948) | 0.2936 | 0.254 | 2 |
SiO2 (mp-32667) | 0.2179 | 0.241 | 2 |
HfO2 (mp-776097) | 0.2592 | 0.028 | 2 |
SrLaMnRuO6 (mp-39239) | 0.7297 | 0.084 | 5 |
SrLaMnRuO6 (mp-690590) | 0.7384 | 0.084 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.7514 eV |
Corrected Energy-161.3786 eV
-161.3786 eV = -138.0339 eV (uncorrected energy) - 19.1310 eV (MP Advanced Correction) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)