Final Magnetic Moment0.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.225 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.234 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3V2P4(HO8)2 + VO2 + Mn2V2O7 + LiMnPO4 + Li3PO4 + H2O |
Band Gap0.298 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 -1> | 279.8 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 219.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 228.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 114.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 335.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 -1> | 167.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 292.3 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 222.4 |
SiO2 (mp-6930) | <0 0 1> | <1 -1 0> | 216.7 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 -1> | 247.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 308.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 0> | 216.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 292.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 266.3 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 269.6 |
LiF (mp-1138) | <1 1 1> | <1 -1 0> | 144.5 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 167.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 266.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 222.4 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 219.2 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 101.9 |
GaN (mp-804) | <1 0 1> | <1 -1 -1> | 247.0 |
GaN (mp-804) | <1 1 0> | <0 1 -1> | 335.8 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 154.1 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 223.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 114.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 277.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 269.6 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 266.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 1> | 242.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 266.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 76.1 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 152.2 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 114.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 114.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 228.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 -1 -1> | 247.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 277.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 -1 -1> | 164.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 269.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 219.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 266.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 266.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 266.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 292.3 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 266.3 |
BN (mp-984) | <0 0 1> | <0 1 -1> | 223.9 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 296.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 266.3 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 279.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2PO5 (mp-770913) | 0.7172 | 0.049 | 3 |
Fe4P2O9 (mp-637226) | 0.6340 | 0.391 | 3 |
Mn4P2O9 (mp-770499) | 0.6231 | 0.015 | 3 |
Cr4P2O9 (mp-773396) | 0.6402 | 0.230 | 3 |
Ni4P2O9 (mp-771899) | 0.6902 | 0.037 | 3 |
Li2V5(PO4)4 (mp-763552) | 0.5725 | 0.062 | 4 |
Li3Sn3(PO4)4 (mp-758156) | 0.6066 | 0.071 | 4 |
Li4Mn2(PO4)3 (mp-764125) | 0.5816 | 0.041 | 4 |
Li3Sb3(PO4)4 (mp-758651) | 0.5215 | 0.064 | 4 |
Li3Sn3(PO4)4 (mp-757551) | 0.5264 | 0.059 | 4 |
LiNiPHO5 (mp-768033) | 0.2883 | 0.155 | 5 |
LiVPHO5 (mp-767213) | 0.2208 | 0.000 | 5 |
LiCrPHO5 (mp-765883) | 0.2725 | 0.000 | 5 |
LiFePHO5 (mp-771864) | 0.2616 | 0.295 | 5 |
LiMnPHO5 (mp-769993) | 0.2138 | 0.000 | 5 |
Li2MnVP2(HO5)2 (mp-849523) | 0.1130 | 0.302 | 6 |
Li2MnVP2(HO5)2 (mp-849423) | 0.0735 | 0.027 | 6 |
Li2MnVP2(HO5)2 (mp-776798) | 0.0948 | 0.104 | 6 |
Li2MnVP2(HO5)2 (mp-778728) | 0.0921 | 0.180 | 6 |
Li2MnVP2(HO5)2 (mp-777091) | 0.1143 | 0.225 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P H O |
Final Energy/Atom-6.5840 eV |
Corrected Energy-257.7946 eV
-257.7946 eV = -237.0231 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 6.7257 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)