Final Magnetic Moment0.101 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.586 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3BiO4 + NaBiO3 + Bi2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 136.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 214.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 258.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 182.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 214.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 299.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 171.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 281.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 281.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 299.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 218.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 214.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 218.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 42.8 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 171.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 109.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 109.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 128.5 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 168.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 281.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 299.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 254.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 327.6 |
BN (mp-984) | <1 1 1> | <0 1 1> | 281.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 134.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 299.8 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 281.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 214.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 291.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 218.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 182.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 182.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 214.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 281.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 134.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 182.0 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 136.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 291.2 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 85.6 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 281.0 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 256.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 214.1 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 214.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 109.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 109.2 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 281.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 134.4 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 168.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 218.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 109.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
EuLu2O4 (mp-984697) | 0.2374 | 0.020 | 3 |
Zn(FeO2)2 (mvc-15076) | 0.2053 | 0.218 | 3 |
MgAl2O4 (mp-5857) | 0.2038 | 0.099 | 3 |
SrGd2O4 (mp-3523) | 0.2516 | 0.011 | 3 |
Mg(FeO2)2 (mvc-15084) | 0.2520 | 0.225 | 3 |
Ca5Sc2(CoO6)2 (mvc-13126) | 0.6894 | 0.027 | 4 |
Ca5Mn2(NiO6)2 (mvc-13112) | 0.7128 | 0.104 | 4 |
Li3CoNi3O8 (mp-764661) | 0.7131 | 0.072 | 4 |
FeBiSbS4 (mp-601716) | 0.7365 | 0.170 | 4 |
Na3Mn4(TeO6)2 (mp-565229) | 0.4015 | 0.000 | 4 |
Cr7Se8 (mp-696673) | 0.7293 | 0.065 | 2 |
V3S4 (mp-850014) | 0.7204 | 0.020 | 2 |
Yb3Se4 (mp-542601) | 0.6909 | 0.219 | 2 |
V3Se4 (mp-22700) | 0.7276 | 0.000 | 2 |
V3S4 (mp-1081) | 0.6930 | 0.020 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Bi O |
Final Energy/Atom-5.3127 eV |
Corrected Energy-159.9932 eV
-159.9932 eV = -148.7566 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)