Final Magnetic Moment0.270 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.817 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.219 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CrO4 + CuO + Cr2O3 |
Band Gap0.524 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 277.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 277.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 294.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 208.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 138.8 |
Fe3O4 (mp-19306) | <1 0 0> | <0 1 0> | 69.4 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 1> | 98.2 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 120.5 |
C (mp-66) | <1 1 0> | <0 1 1> | 196.4 |
PbS (mp-21276) | <1 0 0> | <0 1 0> | 69.4 |
PbS (mp-21276) | <1 1 0> | <0 1 1> | 98.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 1> | 241.0 |
Ga2O3 (mp-886) | <0 1 0> | <0 1 1> | 294.7 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 1> | 294.7 |
Au (mp-81) | <1 0 0> | <0 1 0> | 69.4 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 294.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 208.2 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 279.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 241.0 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 277.6 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 1 0> | 69.4 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 277.6 |
MgAl2O4 (mp-3536) | <1 1 0> | <0 1 1> | 98.2 |
MgAl2O4 (mp-3536) | <1 1 1> | <1 1 1> | 120.5 |
SrTiO3 (mp-4651) | <0 0 1> | <0 1 0> | 277.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 69.4 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 98.2 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 120.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 120.5 |
Cu (mp-30) | <1 0 0> | <0 1 1> | 196.4 |
Cu (mp-30) | <1 1 0> | <0 1 1> | 294.7 |
GaTe (mp-542812) | <0 0 1> | <0 1 1> | 294.7 |
Al (mp-134) | <1 0 0> | <0 1 1> | 98.2 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 196.4 |
Ge (mp-32) | <1 0 0> | <0 1 0> | 69.4 |
LiAlO2 (mp-3427) | <0 0 1> | <0 1 0> | 138.8 |
LiAlO2 (mp-3427) | <1 1 1> | <0 1 0> | 277.6 |
TeO2 (mp-2125) | <1 0 0> | <0 1 1> | 294.7 |
CaF2 (mp-2741) | <1 0 0> | <0 1 0> | 277.6 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 277.6 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 279.1 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 208.2 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 277.6 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 277.6 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 277.6 |
InP (mp-20351) | <1 0 0> | <0 1 0> | 69.4 |
InP (mp-20351) | <1 1 0> | <0 1 1> | 98.2 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 294.7 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 208.2 |
InSb (mp-20012) | <1 1 0> | <0 1 1> | 196.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3Cu3O8 (mp-652534) | 0.1276 | 0.020 | 3 |
Fe9Cu3O16 (mp-868046) | 0.1184 | 0.430 | 3 |
MgMn2O4 (mvc-5228) | 0.1144 | 1.184 | 3 |
Mn5(FeO3)4 (mp-763271) | 0.1170 | 0.072 | 3 |
LiCr2O4 (mp-774032) | 0.0846 | 0.048 | 3 |
Li2Cr3FeO8 (mp-777653) | 0.0938 | 0.860 | 4 |
Li2MnCr3O8 (mp-774951) | 0.0973 | 0.005 | 4 |
Li2FeCo3O8 (mp-761944) | 0.0835 | 0.000 | 4 |
Li2CrCo3O8 (mp-762609) | 0.0880 | 0.068 | 4 |
Li2V3CrO8 (mp-774288) | 0.1055 | 0.003 | 4 |
Hf3N4 (mp-755988) | 0.2836 | 0.016 | 2 |
In3S4 (mp-556597) | 0.2630 | 0.042 | 2 |
Ni3S4 (mp-1050) | 0.2557 | 0.000 | 2 |
Sn3N4 (mp-16031) | 0.2674 | 0.000 | 2 |
Ge3N4 (mp-476) | 0.2779 | 0.109 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.2427 | 0.897 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.1628 | 0.014 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.2007 | 0.069 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.2427 | 0.035 | 5 |
TaTi9Al3Zn23O48 (mp-695545) | 0.2334 | 0.054 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7157 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7187 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7240 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7186 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7227 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Cu_pv O |
Final Energy/Atom-6.4457 eV |
Corrected Energy-407.5906 eV
-407.5906 eV = -360.9613 eV (uncorrected energy) - 24.1560 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)