Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.280 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.093 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi5FeO4 + Li2FeO3 + Li2O2 + LiF |
Band Gap1.019 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 157.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 220.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 157.4 |
LaAlO3 (mp-2920) | <1 1 1> | <1 -1 -1> | 258.0 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 129.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 107.9 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 126.0 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 188.9 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 259.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 242.7 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 126.0 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 162.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 94.5 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 162.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 346.4 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 157.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 215.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 188.8 |
GaN (mp-804) | <1 1 0> | <1 -1 -1> | 206.4 |
GaN (mp-804) | <1 1 1> | <1 -1 -1> | 154.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 305.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 188.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 80.9 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 94.5 |
LiF (mp-1138) | <1 1 1> | <0 1 1> | 283.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 138.8 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 94.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 305.4 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 162.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 302.8 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 260.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 242.7 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 259.7 |
YVO4 (mp-19133) | <1 0 0> | <1 -1 -1> | 309.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 291.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 31.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 129.8 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 157.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 94.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 53.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 64.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 220.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 134.8 |
TePb (mp-19717) | <1 1 0> | <1 1 -1> | 313.2 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 350.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 94.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 188.9 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 86.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co(NiS2)2 (mp-674858) | 0.5186 | 0.113 | 3 |
Li4FeO4 (mp-769843) | 0.5521 | 0.080 | 3 |
Li2BiS3 (mp-768229) | 0.5678 | 0.073 | 3 |
LiMnO2 (mp-25542) | 0.5317 | 0.022 | 3 |
CaCoO2 (mvc-13795) | 0.4848 | 0.274 | 3 |
Li4Mn(OF)2 (mp-767317) | 0.5845 | 0.092 | 4 |
Li6FeO5F (mp-765049) | 0.4102 | 0.088 | 4 |
Li5VO4F (mp-764217) | 0.5902 | 0.048 | 4 |
Li7Mn(O2F)2 (mp-767185) | 0.6221 | 0.065 | 4 |
Li6MnAlO6 (mp-770706) | 0.6015 | 0.121 | 4 |
Nb4O5 (mp-28212) | 0.6231 | 0.024 | 2 |
Sr4N3 (mp-685023) | 0.5932 | 0.191 | 2 |
Cr3N4 (mp-1014365) | 0.6479 | 0.191 | 2 |
Tc2P3 (mp-9895) | 0.5582 | 0.000 | 2 |
Tc2P3 (mp-11690) | 0.6518 | 0.006 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.1277 eV |
Corrected Energy-144.4035 eV
-144.4035 eV = -133.3192 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)