material

CeScO3

ID:

mp-777413

DOI:

10.17188/1272671


Tags: Cerium trioxoscandate

Material Details

Final Magnetic Moment
1.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-3.856 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.013 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.83 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ce2O3 + Sc2O3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 195596 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Plane
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 0 0> <1 1 0> 0.011 327.3
Cu (mp-30) <1 0 0> <1 1 0> 0.011 65.5
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.012 131.6
YVO4 (mp-19133) <0 0 1> <1 1 0> 0.015 261.8
SiC (mp-8062) <1 0 0> <1 1 0> 0.022 327.3
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.022 131.6
TiO2 (mp-390) <0 0 1> <1 1 0> 0.024 130.9
CdS (mp-672) <1 0 0> <0 1 0> 0.025 318.3
ZnSe (mp-1190) <1 1 1> <0 1 0> 0.036 227.3
Ga2O3 (mp-886) <0 1 0> <1 0 0> 0.046 141.3
GaAs (mp-2534) <1 1 1> <0 1 0> 0.060 227.3
Cu (mp-30) <1 1 1> <0 0 1> 0.062 361.9
TePb (mp-19717) <1 1 0> <0 1 0> 0.072 181.9
BN (mp-984) <1 1 1> <1 0 0> 0.078 235.5
TeO2 (mp-2125) <1 1 0> <1 1 0> 0.079 196.4
CdS (mp-672) <1 1 1> <1 1 0> 0.080 261.8
BaTiO3 (mp-5986) <1 0 0> <0 1 0> 0.085 136.4
NaCl (mp-22862) <1 1 0> <0 1 0> 0.091 45.5
DyScO3 (mp-31120) <0 1 0> <1 1 0> 0.095 130.9
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.102 197.4
CdS (mp-672) <1 0 1> <0 1 0> 0.105 227.3
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.106 47.1
Ge (mp-32) <1 1 1> <0 1 0> 0.121 227.3
LaAlO3 (mp-2920) <0 0 1> <1 0 0> 0.122 329.6
ZnO (mp-2133) <0 0 1> <0 1 1> 0.123 56.1
C (mp-48) <0 0 1> <0 1 1> 0.125 168.4
LiGaO2 (mp-5854) <1 1 0> <0 1 1> 0.127 336.8
KTaO3 (mp-3614) <1 1 1> <0 1 1> 0.129 56.1
C (mp-48) <1 0 1> <1 1 0> 0.129 261.8
AlN (mp-661) <1 0 0> <1 1 1> 0.133 219.8
KTaO3 (mp-3614) <1 1 0> <0 1 0> 0.135 45.5
TiO2 (mp-390) <1 0 1> <0 0 1> 0.144 361.9
NaCl (mp-22862) <1 1 1> <0 1 0> 0.145 227.3
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.149 361.9
Al (mp-134) <1 1 1> <0 1 1> 0.162 56.1
Au (mp-81) <1 1 0> <0 0 1> 0.171 98.7
ZnO (mp-2133) <1 1 0> <0 1 0> 0.172 90.9
TeO2 (mp-2125) <0 1 0> <0 1 0> 0.187 136.4
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.194 164.5
ZnO (mp-2133) <1 1 1> <0 1 1> 0.205 224.5
C (mp-66) <1 1 0> <0 0 1> 0.208 197.4
Te2W (mp-22693) <0 1 1> <0 0 1> 0.211 296.1
Ag (mp-124) <1 1 0> <0 0 1> 0.211 98.7
Al (mp-134) <1 1 0> <0 1 0> 0.213 45.5
LiGaO2 (mp-5854) <1 1 1> <1 1 1> 0.214 219.8
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.218 57.4
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.218 57.4
GaSe (mp-1943) <0 0 1> <0 1 1> 0.239 112.3
Ag (mp-124) <1 1 1> <1 0 0> 0.251 235.5
BN (mp-984) <0 0 1> <1 1 1> 0.251 219.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
259 103 119 0 0 0
103 232 102 0 0 0
119 102 261 0 0 0
0 0 0 74 0 0
0 0 0 0 72 0
0 0 0 0 0 81
Compliance Tensor Sij (10-12Pa-1)
5.3 -1.6 -1.8 0 0 0
-1.6 5.7 -1.5 0 0 0
-1.8 -1.5 5.2 0 0 0
0 0 0 13.4 0 0
0 0 0 0 13.9 0
0 0 0 0 0 12.3
Shear Modulus GV
74 GPa
Bulk Modulus KV
156 GPa
Shear Modulus GR
74 GPa
Bulk Modulus KR
154 GPa
Shear Modulus GVRH
74 GPa
Bulk Modulus KVRH
155 GPa
Elastic Anisotropy
0.03
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NdScO3 (mp-31117) 0.0682 0.000 3
EuScO3 (mp-22487) 0.0339 0.044 3
NaCoF3 (mp-555201) 0.0850 0.000 3
CaZrO3 (mp-4571) 0.0859 0.000 3
CaSnO3 (mp-4438) 0.0856 0.014 3
Ca2SnIrO6 (mvc-5666) 0.1226 0.067 4
Ca2SnSbO6 (mvc-3972) 0.0980 0.076 4
Ca2TiSbO6 (mvc-3961) 0.1986 0.092 4
Ca4Zr3TaO12 (mp-756837) 0.1881 0.033 4
CaPr(SnO3)2 (mvc-9344) 0.1474 0.133 4
U2S3 (mp-672690) 0.6625 0.173 2
Al2O3 (mp-642363) 0.5857 0.280 2
Cr3C2 (mp-570112) 0.6405 0.030 2
Ga2O3 (mp-13134) 0.6843 0.284 2
Fe2O3 (mp-1078361) 0.6718 0.236 2
LiLaNdSbO6 (mp-776091) 0.2701 0.006 5
LaMgFeSnO6 (mvc-9082) 0.2787 0.126 5
LaMgCrMoO6 (mvc-9867) 0.2872 0.714 5
LaMgCrSbO6 (mvc-9859) 0.2690 0.842 5
LaMgCrSnO6 (mvc-9925) 0.2611 0.763 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ce Sc_sv O
Final Energy/Atom
-8.8655 eV
Corrected Energy
-185.5534 eV
Uncorrected energy = -177.3094 eV Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV Corrected energy = -185.5534 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 195596
Submitted by
User remarks:
  • Cerium trioxoscandate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)