Final Magnetic Moment6.018 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.504 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.39 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToP3(WO6)2 + Li3PO4 + W |
Band Gap3.674 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 327.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 196.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 196.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 327.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 327.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 261.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 196.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 196.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 196.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 261.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 261.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 261.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 196.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 196.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 130.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 196.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 327.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 196.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 196.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.5 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 327.3 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 327.3 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 261.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 327.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 261.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 65.5 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 196.4 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.5 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 261.8 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 261.8 |
Si (mp-149) | <1 1 0> | <0 0 1> | 327.3 |
Si (mp-149) | <1 1 1> | <0 0 1> | 196.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 261.8 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 196.4 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 65.5 |
C (mp-48) | <0 0 1> | <0 0 1> | 196.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 261.8 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 261.8 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 261.8 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 196.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 65.5 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 261.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YTcN3 (mp-989640) | 0.4343 | 0.021 | 3 |
YReN3 (mp-989628) | 0.4425 | 0.009 | 3 |
CaReN3 (mp-989606) | 0.4452 | 0.000 | 3 |
PRhO4 (mp-28870) | 0.4235 | 0.000 | 3 |
Ni7(PO4)6 (mp-32385) | 0.4655 | 0.102 | 3 |
Li3Cu2(SO4)3 (mp-778458) | 0.1860 | 0.045 | 4 |
Li3In2(PO4)3 (mp-6425) | 0.1230 | 0.003 | 4 |
Li3V2(PO4)3 (mp-850900) | 0.2207 | 0.019 | 4 |
Li3Mo2(PO4)3 (mp-32098) | 0.0962 | 0.000 | 4 |
Li3Ni2(PO4)3 (mp-504228) | 0.1806 | 0.054 | 4 |
CrO2 (mvc-11581) | 0.7431 | 0.166 | 2 |
VO2 (mp-777469) | 0.6614 | 0.038 | 2 |
VO2 (mvc-6918) | 0.6669 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.5878 | 0.281 | 2 |
Li6MnV3(PO4)6 (mp-779201) | 0.2790 | 0.021 | 5 |
Li3MnV(PO4)3 (mp-778888) | 0.3050 | 0.044 | 5 |
Li3MnV(PO4)3 (mp-778788) | 0.2845 | 0.146 | 5 |
Li4MnV(PO4)3 (mp-770136) | 0.2921 | 0.198 | 5 |
Li3MnV(PO4)3 (mp-774297) | 0.3040 | 0.192 | 5 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.5752 | 0.086 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5503 | 0.080 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5821 | 0.020 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.5228 | 0.008 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.5571 | 0.778 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv P W_pv O |
Final Energy/Atom-7.0109 eV |
Corrected Energy-314.6939 eV
-314.6939 eV = -280.4350 eV (uncorrected energy) - 17.4040 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)