Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.935 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.414 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiF + FeF2 |
Band Gap3.587 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 52.4 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 209.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 308.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 261.8 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 84.6 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 123.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 185.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 228.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 260.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 130.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 195.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 185.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 185.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 312.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 185.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 314.2 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 234.1 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 246.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 260.5 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 185.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 358.3 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 209.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 173.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 97.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 325.7 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 308.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 173.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 52.4 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 209.4 |
MoS2 (mp-1434) | <1 1 1> | <0 0 1> | 228.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 162.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 231.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 104.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 130.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 289.3 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 261.8 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 261.8 |
CdTe (mp-406) | <1 1 1> | <0 1 0> | 157.1 |
TeO2 (mp-2125) | <0 1 1> | <0 1 1> | 308.3 |
TeO2 (mp-2125) | <1 0 1> | <0 1 1> | 308.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 130.3 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 261.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 97.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 228.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 130.3 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 195.4 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 260.5 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 209.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 228.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 289.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2VF4 (mp-776767) | 0.4013 | 0.184 | 3 |
Li2Mn3F8 (mp-766722) | 0.4091 | 0.058 | 3 |
LiBiO3 (mp-29077) | 0.4084 | 0.000 | 3 |
Li2FeF5 (mp-776886) | 0.4105 | 0.026 | 3 |
Li2VF4 (mp-778294) | 0.4033 | 0.199 | 3 |
Li2V2OF5 (mp-765272) | 0.3428 | 0.074 | 4 |
Li4Fe(TeO4)3 (mp-777889) | 0.3381 | 0.214 | 4 |
Li4V4(OF3)3 (mp-765901) | 0.3239 | 0.101 | 4 |
Li4Mn(TeO4)3 (mp-771794) | 0.3276 | 0.065 | 4 |
Ca4Ni5(TeO6)3 (mvc-3151) | 0.3641 | 0.193 | 4 |
V3O5 (mp-714911) | 0.4522 | 0.003 | 2 |
V3O5 (mp-542441) | 0.4301 | 0.029 | 2 |
Ti3O5 (mp-556754) | 0.4484 | 0.013 | 2 |
Ti4O7 (mp-12205) | 0.4346 | 0.007 | 2 |
Ti4O7 (mp-558097) | 0.4390 | 0.007 | 2 |
Li4CrTe2WO12 (mp-775509) | 0.3126 | 0.109 | 5 |
Li4NbFe(WO6)2 (mp-850102) | 0.3136 | 0.019 | 5 |
Li4NbCr(WO6)2 (mp-769739) | 0.3107 | 0.023 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.3078 | 0.036 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.3116 | 0.076 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv F |
Final Energy/Atom-4.7676 eV |
Corrected Energy-149.9094 eV
Uncorrected energy = -133.4934 eV
Composition-based energy adjustment (-0.462 eV/atom x 16.0 atoms) = -7.3920 eV
Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV
Corrected energy = -149.9094 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)