Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.042 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.081 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVF4 + LiV3(OF3)2 |
Band Gap1.670 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 114.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 283.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 114.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 101.5 |
CdS (mp-672) | <0 0 1> | <1 -1 1> | 231.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 283.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 283.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 158.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 283.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 203.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 203.0 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 158.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 203.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 283.3 |
BN (mp-984) | <1 0 0> | <1 -1 1> | 115.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 94.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 283.3 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 158.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 94.4 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 283.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 283.3 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 229.0 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 94.4 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 203.0 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 0> | 114.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 1> | 158.2 |
C (mp-66) | <1 0 0> | <1 -1 1> | 115.9 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 114.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 229.0 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 283.3 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 114.5 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 283.3 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 283.3 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 283.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 114.5 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 283.3 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 114.5 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 1> | 158.2 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 94.4 |
YAlO3 (mp-3792) | <1 0 0> | <1 -1 -1> | 158.8 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 283.3 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 1> | 183.6 |
TiO2 (mp-390) | <1 0 1> | <1 0 -1> | 115.8 |
TiO2 (mp-390) | <0 0 1> | <1 -1 1> | 115.9 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 283.3 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 283.3 |
GaTe (mp-542812) | <0 1 0> | <1 1 0> | 190.8 |
GaTe (mp-542812) | <1 0 0> | <0 1 0> | 229.0 |
Cu (mp-30) | <1 1 0> | <0 1 1> | 183.6 |
Fe2O3 (mp-24972) | <0 0 1> | <0 1 1> | 183.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiVF4 (mp-764895) | 0.5902 | 0.024 | 3 |
LiMnF4 (mp-778553) | 0.5434 | 0.059 | 3 |
V(SbO3)4 (mp-770857) | 0.5900 | 0.046 | 3 |
Li2MnF6 (mp-766903) | 0.5970 | 0.158 | 3 |
Mn(SbO3)4 (mp-773338) | 0.5729 | 0.037 | 3 |
LiV2OF5 (mp-783911) | 0.3154 | 0.083 | 4 |
LiV2OF5 (mp-853273) | 0.3263 | 0.186 | 4 |
LiV2OF5 (mp-850443) | 0.2868 | 0.094 | 4 |
LiV2OF5 (mp-777084) | 0.2255 | 0.230 | 4 |
LiV2OF5 (mp-778300) | 0.3548 | 0.105 | 4 |
Ba3LiTa3Ti5O21 (mp-677212) | 0.6585 | 0.000 | 5 |
Ba3LiTi5Nb3O21 (mp-766208) | 0.6933 | 0.010 | 5 |
Li7Zr3Nb(TeO6)4 (mp-766103) | 0.6405 | 0.012 | 5 |
Li3ZrNb(TeO6)2 (mp-754249) | 0.4878 | 0.021 | 5 |
Ba6Li2Ti7Nb9O42 (mp-773084) | 0.6919 | 0.011 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-6.1597 eV |
Corrected Energy-476.0291 eV
-476.0291 eV = -443.4988 eV (uncorrected energy) - 26.9120 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)