Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.474 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.531 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.45 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeF2 + LiF |
Band Gap3.596 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 300.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 246.2 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 101.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 109.4 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 118.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 326.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 326.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 300.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 161.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 237.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 267.0 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 267.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 218.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 101.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 191.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 291.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 328.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 89.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 356.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 148.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 242.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 101.0 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 296.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 161.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 207.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 237.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 54.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 328.3 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 282.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 267.0 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 267.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 161.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 237.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 80.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 118.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 322.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 246.2 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 121.1 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 191.5 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 201.8 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 201.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 118.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 118.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 291.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 202.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 267.0 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 207.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 328.3 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 136.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 194.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2N2O (mp-760052) | 0.4898 | 0.100 | 3 |
Zn(CoO2)2 (mvc-12655) | 0.4562 | 0.189 | 3 |
Mg(WO2)2 (mvc-5982) | 0.3682 | 0.511 | 3 |
Mg(MoO2)2 (mvc-6043) | 0.3764 | 0.305 | 3 |
Ca2SnS4 (mp-866539) | 0.3374 | 0.314 | 3 |
Li7VO5F (mp-764775) | 0.6386 | 0.067 | 4 |
Li7Mn(OF)3 (mp-764343) | 0.6373 | 0.085 | 4 |
Li7Mn(OF)3 (mp-767191) | 0.6561 | 0.273 | 4 |
Li7V(O2F)2 (mp-765831) | 0.6504 | 0.103 | 4 |
KCu(BiS2)2 (mp-558063) | 0.6362 | 0.000 | 4 |
Ca3N2 (mp-568172) | 0.5204 | 0.048 | 2 |
Sc2O3 (mp-558748) | 0.4687 | 0.074 | 2 |
Lu2O3 (mp-556477) | 0.5113 | 0.057 | 2 |
Tm2O3 (mp-556253) | 0.5212 | 0.051 | 2 |
Er2O3 (mp-2460) | 0.5238 | 0.048 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv F |
Final Energy/Atom-4.6509 eV |
Corrected Energy-141.1581 eV
-141.1581 eV = -130.2261 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction)
|