Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.421 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.79 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 + Li2Ti3CoO8 + SnO2 |
Band Gap0.264 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 231.4 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 249.8 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 114.1 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 257.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 173.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 114.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 239.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 114.1 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 289.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.6 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 57.8 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 289.2 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 196.7 |
LiTaO3 (mp-3666) | <1 0 1> | <1 1 0> | 228.2 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 249.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 179.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 173.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 173.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 59.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 179.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 179.4 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 231.4 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 57.8 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 114.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 289.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 239.2 |
LiNbO3 (mp-3731) | <1 0 1> | <1 1 0> | 228.2 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 173.5 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 249.8 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 173.5 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 231.4 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 57.8 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 98.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 173.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 239.2 |
Al (mp-134) | <1 1 1> | <1 1 0> | 114.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 231.4 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 115.7 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 179.4 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 231.4 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 289.2 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 231.4 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 289.2 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 173.5 |
MgO (mp-1265) | <1 1 1> | <1 0 1> | 249.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 83.3 |
Au (mp-81) | <1 0 0> | <1 0 0> | 173.5 |
Au (mp-81) | <1 1 0> | <1 0 0> | 173.5 |
Au (mp-81) | <1 1 1> | <0 0 1> | 59.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 179.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.2420 | 0.074 | 3 |
Ca(AgO2)2 (mvc-5243) | 0.2452 | 0.235 | 3 |
Ca(AgO2)2 (mvc-4859) | 0.2285 | 0.228 | 3 |
LiFe5O8 (mp-706252) | 0.2415 | 0.099 | 3 |
Zn(SnO2)2 (mvc-9533) | 0.2410 | 0.247 | 3 |
Li4Co3Ni5O16 (mp-772319) | 0.1889 | 0.035 | 4 |
Li4Ti3Mn5O16 (mp-773545) | 0.1725 | 0.045 | 4 |
Li4Fe5Co3O16 (mp-773387) | 0.1889 | 0.058 | 4 |
Li4Fe3Ni5O16 (mp-773324) | 0.1830 | 0.115 | 4 |
Li4Mn5Co3O16 (mp-771231) | 0.1860 | 0.039 | 4 |
Si3N4 (mp-641539) | 0.3593 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.3314 | 0.208 | 2 |
Fe3O4 (mp-542433) | 0.3545 | 0.072 | 2 |
Fe3O4 (mp-650112) | 0.3228 | 0.057 | 2 |
Fe3O4 (mp-715558) | 0.3700 | 0.076 | 2 |
Li4Fe2Co3Ni3O16 (mp-775701) | 0.1453 | 0.042 | 5 |
Li4Mn3Cu3(SnO8)2 (mp-775474) | 0.1401 | 0.043 | 5 |
Li4Ti3Co3(NiO8)2 (mp-763517) | 0.1342 | 0.058 | 5 |
Li4Ti3Ni3(SnO8)2 (mp-851029) | 0.0976 | 0.032 | 5 |
Li4Mn3Co3(TeO8)2 (mp-769585) | 0.1341 | 0.008 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7440 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Co Sn_d O |
Final Energy/Atom-6.8127 eV |
Corrected Energy-207.6149 eV
-207.6149 eV = -190.7562 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 5.6220 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)