Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.555 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.034 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeO + FeF2 + LiF |
Band Gap2.906 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 291.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 170.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 291.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 194.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 271.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 323.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 161.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 161.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 355.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 194.0 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 189.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 226.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 355.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 355.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 327.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 252.8 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 316.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 161.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 226.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 291.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 255.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 161.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 271.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 323.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 226.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 271.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 226.4 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 291.9 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 217.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 226.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 64.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 327.2 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 170.1 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 97.0 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 97.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 258.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 226.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 64.7 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 252.8 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 217.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 65.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 327.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 327.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 97.0 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 196.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 258.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 355.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 217.2 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 291.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2UO4 (mp-9607) | 0.2947 | 0.000 | 3 |
Mn2GeS4 (mp-621925) | 0.3785 | 0.043 | 3 |
Li2ZnCl4 (mp-23416) | 0.3807 | 0.013 | 3 |
Zn7(SbO6)2 (mp-675797) | 0.3743 | 0.009 | 3 |
Fe2GeS4 (mp-21086) | 0.3793 | 0.155 | 3 |
LiMn2OF3 (mp-767309) | 0.1426 | 0.053 | 4 |
Li2Mn3VO8 (mp-781772) | 0.3201 | 0.059 | 4 |
LiFe2OF3 (mp-764580) | 0.3153 | 0.051 | 4 |
LiNiSbO4 (mp-1094134) | 0.2747 | 0.184 | 4 |
LiCo2OF3 (mp-765692) | 0.2170 | 0.083 | 4 |
Fe3O4 (mp-715491) | 0.4813 | 0.015 | 2 |
Si3N4 (mp-641539) | 0.4506 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4556 | 0.208 | 2 |
Mn3N4 (mp-1080204) | 0.4478 | 0.073 | 2 |
Cr3N4 (mp-1014358) | 0.4319 | 0.227 | 2 |
Li4Co3Ni3(WO8)2 (mp-764321) | 0.3103 | 0.061 | 5 |
Li4V3Ni3(WO8)2 (mp-777059) | 0.3238 | 0.032 | 5 |
Li4Cr3Ni3(WO8)2 (mp-761720) | 0.3251 | 0.033 | 5 |
Li4Fe3Co3(WO8)2 (mp-776860) | 0.3276 | 0.056 | 5 |
Li4V3Co3(WO8)2 (mp-763152) | 0.3080 | 0.263 | 5 |
Li3MnFeCo(PO4)3 (mp-764804) | 0.6950 | 0.030 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6907 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6966 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7004 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6931 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.6826 eV |
Corrected Energy-183.7864 eV
-183.7864 eV = -159.1132 eV (uncorrected energy) - 21.8640 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)