Final Magnetic Moment3.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.843 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn2TeO6 + Li2TeO4 + TeO2 |
Band Gap0.389 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2 [3] |
HallP 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 287.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 263.0 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 175.3 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 193.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 219.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 313.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 261.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 306.8 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 261.3 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 204.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 219.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 131.5 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 204.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 135.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 234.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 226.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 219.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 43.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 219.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 246.2 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 193.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 306.8 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 204.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 261.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 278.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 255.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 131.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 255.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 130.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 234.9 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 322.1 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 234.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 130.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 261.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 226.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 219.1 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 306.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 263.0 |
YVO4 (mp-19133) | <1 0 0> | <1 1 -1> | 133.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 130.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 87.7 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 313.2 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 153.0 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 257.7 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 234.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 234.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 87.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 130.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 263.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 87.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.41460 | 0.00000 | -0.08969 |
-0.31389 | 1.16367 | 0.65319 | 0.00000 | 0.29280 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.24227 | 0.00000 | 0.21037 |
Piezoelectric Modulus ‖eij‖max1.40180 C/m2 |
Crystallographic Direction vmax |
---|
-0.00000 |
-2.00000 |
-1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.35 | 0.00 | -0.13 |
0.00 | 6.62 | 0.00 |
-0.13 | 0.00 | 4.57 |
Dielectric Tensor εij (total) |
||
---|---|---|
21.88 | 0.00 | 1.37 |
0.00 | 23.11 | 0.00 |
1.37 | 0.00 | 14.81 |
Polycrystalline dielectric constant
εpoly∞
5.85
|
Polycrystalline dielectric constant
εpoly
19.93
|
Refractive Index n2.42 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Al2SiO5 (mp-9515) | 0.4269 | 0.100 | 3 |
MgSbO3 (mvc-15602) | 0.4289 | 0.159 | 3 |
LiTeO3 (mp-755231) | 0.3066 | 0.063 | 3 |
Li2FeF5 (mp-776886) | 0.3987 | 0.031 | 3 |
Li2Fe3F8 (mp-776754) | 0.4249 | 0.026 | 3 |
Li4Ti(TeO4)3 (mp-850190) | 0.2696 | 0.030 | 4 |
Li4V(TeO4)3 (mp-779999) | 0.1068 | 0.036 | 4 |
Li4Nb(TeO4)3 (mp-756515) | 0.2327 | 0.085 | 4 |
Li4Fe(TeO4)3 (mp-776188) | 0.2383 | 0.184 | 4 |
Li4Nb(FeO4)3 (mp-774238) | 0.2974 | 0.139 | 4 |
V3O5 (mp-542441) | 0.4250 | 0.029 | 2 |
Mn5O8 (mp-18922) | 0.4525 | 0.009 | 2 |
Ti4O7 (mp-12205) | 0.4575 | 0.005 | 2 |
Mn5O8 (mp-715008) | 0.4439 | 0.009 | 2 |
Ti4O7 (mp-558097) | 0.4521 | 0.005 | 2 |
Li4MnSn(WO6)2 (mp-775961) | 0.3619 | 0.051 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.3389 | 0.035 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.3606 | 0.076 | 5 |
Li4VCr(TeO6)2 (mp-771088) | 0.4014 | 0.068 | 5 |
Li4TiMn(WO6)2 (mp-770980) | 0.4109 | 0.032 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Te O |
Final Energy/Atom-5.6182 eV |
Corrected Energy-122.4726 eV
-122.4726 eV = -112.3643 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 1.6809 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)