Final Magnetic Moment0.084 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.816 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.263 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2O3 + LiF + LiV3(OF3)2 |
Band Gap0.595 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 256.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 142.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 313.2 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 256.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 85.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 170.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 252.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 341.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 87.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 370.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 261.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 256.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 28.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 370.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 241.0 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 199.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 341.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 227.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 341.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 -1> | 254.4 |
GaSe (mp-1943) | <1 0 0> | <0 1 -1> | 279.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 170.8 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 279.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 142.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 370.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 28.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 168.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 142.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 241.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 256.2 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 199.3 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 227.8 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 91.6 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 341.6 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 341.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 227.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 227.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 1> | 183.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 313.2 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 113.9 |
C (mp-66) | <1 0 0> | <0 1 1> | 252.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 56.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 313.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 227.8 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 85.4 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 252.1 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 -1> | 279.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 142.4 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 84.0 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 256.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3VF6 (mp-622187) | 0.4609 | 0.143 | 3 |
Li3MnF6 (mp-763801) | 0.4230 | 0.131 | 3 |
Li3TiF6 (mp-21540) | 0.4152 | 0.000 | 3 |
Li3VF6 (mp-558578) | 0.4619 | 0.143 | 3 |
Li3AlF6 (mp-15254) | 0.4739 | 0.000 | 3 |
Li11V6O5F19 (mp-850254) | 0.3505 | 0.058 | 4 |
Li11V6O5F19 (mp-779345) | 0.4421 | 0.167 | 4 |
Li11V6O5F19 (mp-780480) | 0.3902 | 0.068 | 4 |
Li11V6O5F19 (mp-777941) | 0.3230 | 0.075 | 4 |
Mg4Fe5(TeO6)3 (mvc-3101) | 0.3976 | 0.491 | 4 |
Fe2O3 (mp-628327) | 0.7059 | 0.749 | 2 |
V3O5 (mp-622497) | 0.7168 | 0.004 | 2 |
V5O9 (mp-714932) | 0.6633 | 0.017 | 2 |
V5O9 (mp-558587) | 0.7051 | 0.008 | 2 |
Ti4O7 (mp-558097) | 0.7166 | 0.005 | 2 |
Li4FeTe(WO6)2 (mp-771716) | 0.6405 | 0.163 | 5 |
Li4MnNb2WO12 (mp-771475) | 0.5832 | 0.046 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.6365 | 0.109 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.6345 | 0.041 | 5 |
Li4FeTe2WO12 (mp-775176) | 0.6333 | 0.208 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.5876 eV |
Corrected Energy-242.6950 eV
-242.6950 eV = -229.0916 eV (uncorrected energy) - 10.0920 eV (MP Advanced Correction) - 3.5114 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)