Final Magnetic Moment35.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.450 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnBO3 + LiFeBO3 |
Band Gap3.095 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 283.6 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 171.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 126.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 220.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 283.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 283.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 346.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 252.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 283.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 220.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 283.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 220.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 252.1 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 256.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 220.6 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 315.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 84.7 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 86.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 220.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 254.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 220.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 252.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 157.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 252.1 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 257.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 252.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 157.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 202.6 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 169.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 315.2 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 252.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 315.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 252.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 189.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 254.1 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 283.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 220.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 220.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 252.1 |
BN (mp-984) | <1 1 1> | <0 0 1> | 315.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 315.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 283.6 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 283.6 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 84.7 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 346.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 252.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 157.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 283.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 84.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 169.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiNiBO3 (mp-761322) | 0.3533 | 0.035 | 4 |
LiCoBO3 (mp-766795) | 0.3719 | 0.000 | 4 |
LiMnBO3 (mp-849500) | 0.3420 | 0.005 | 4 |
LiMnBO3 (mp-769813) | 0.1182 | 0.005 | 4 |
LiFeBO3 (mp-783910) | 0.3086 | 0.000 | 4 |
Li3BO3 (mp-27275) | 0.6292 | 0.000 | 3 |
Li2MnF4 (mp-764846) | 0.6187 | 0.060 | 3 |
Na3CoO3 (mp-777919) | 0.5579 | 0.018 | 3 |
Li2FeF4 (mp-778532) | 0.6010 | 0.057 | 3 |
Li6B4O9 (mp-1020024) | 0.6074 | 0.000 | 3 |
Li8Mn3Fe5(BO3)8 (mp-779373) | 0.0255 | 0.005 | 5 |
Li8Mn5Fe3(BO3)8 (mp-780799) | 0.0372 | 0.005 | 5 |
Li4Mn3Fe(BO3)4 (mp-775239) | 0.0362 | 0.005 | 5 |
Li8Mn5Fe3(BO3)8 (mp-780436) | 0.0306 | 0.005 | 5 |
Li4MnFe3(BO3)4 (mp-778926) | 0.0287 | 0.004 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points16 |
U ValuesFe: 5.3 eVMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Fe_pv B O |
Final Energy/Atom-7.0617 eV |
Corrected Energy-374.5261 eV
-374.5261 eV = -338.9636 eV (uncorrected energy) - 18.7076 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)